Search
×
FR

Placeholder headline

This is just a placeholder headline

API STD 521: Guide for Pressure-relieving and Depressuring Systems – Edition 6

$

682

BUY NOW

Placeholder headline

This is just a placeholder headline

API STD 653: Tank Inspection, Repair, Alteration, and Reconstruction – Edition 4

$

507

BUY NOW

Placeholder headline

This is just a placeholder headline

CSA Z662:19 – Oil and gas pipeline systems

$

1197

BUY NOW

Placeholder headline

This is just a placeholder headline

CSA Z341 Series-18: Storage of hydrocarbons in underground formations

$

878

BUY NOW

Placeholder headline

This is just a placeholder headline

CSA Z246.2-14 – Emergency preparedness and response for petroleum and natural gas industry systems

$

596

BUY NOW

Placeholder headline

This is just a placeholder headline

CSA Z341 Series:22 – Storage of hydrocarbons in underground formations

$

878

BUY NOW

Placeholder headline

This is just a placeholder headline

CSA Z731-09 (R2014) – Emergency Preparedness and Response

$

177

BUY NOW

Placeholder headline

This is just a placeholder headline

CSA Z662:23 – Oil and gas pipeline systems

$

1197

BUY NOW

Placeholder headline

This is just a placeholder headline

CSA Z341 Series:26 – Storage of Hydrocarbons in underground formations

$

878

BUY NOW

Placeholder headline

This is just a placeholder headline

CSA B51:24 Boiler, Pressure Vessel, and Pressure Piping Code

$

389

BUY NOW

ISO 2566:2021

ISO 2566:2021 Steel – Conversion of elongation values – Part 1: Carbon and low-alloy steels

CDN $295.00

SKU: b60a7bca9eef Categories: ,

Description

This document specifies a method of converting room temperature percentage elongations after fracture obtained on various proportional and non-proportional gauge lengths to other gauge lengths.

Formula (1), on which conversions are based, is considered to be reliable when applied to carbon, carbon manganese, molybdenum and chromium molybdenum steels within the tensile strength range 300 N/mm2 to 700 N/mm2 and in the hot-rolled, hot-rolled and normalized or annealed conditions, with or without tempering.

These conversions are not applicable to:

a) cold reduced steels;

b) quenched and tempered steels;

c) austenitic steels.

These conversions are not applicable when the gauge length exceeds  or where the width to thickness ratio of the test piece exceeds 20.

Edition

3

Published Date

2021-12-15

Status

PUBLISHED

Pages

33

Language Detail Icon

English

Format Secure Icon

Secure PDF

Abstract

This document specifies a method of converting room temperature percentage elongations after fracture obtained on various proportional and non-proportional gauge lengths to other gauge lengths.

Formula (1), on which conversions are based, is considered to be reliable when applied to carbon, carbon manganese, molybdenum and chromium molybdenum steels within the tensile strength range 300 N/mm2 to 700 N/mm2 and in the hot-rolled, hot-rolled and normalized or annealed conditions, with or without tempering.

These conversions are not applicable to:

a) cold reduced steels;

b) quenched and tempered steels;

c) austenitic steels.

These conversions are not applicable when the gauge length exceeds  or where the width to thickness ratio of the test piece exceeds 20.