ISO 6892:2015

ISO 6892:2015 Metallic materials – Tensile testing – Part 4: Method of test in liquid helium

CDN $195.00

SKU: ee9be24ba034 Category:

Description

ISO 6892-4:2015 specifies the method of tensile testing of metallic materials in liquid helium (the boiling point is ?269 °C or 4,2 K, designated as 4 K) and defines the mechanical properties that can be determined.

This part of ISO 6892 may apply also to tensile testing at cryogenic temperatures (less than ?196 °C or 77 K), which requires special apparatus, smaller test pieces, and concern for serrated yielding, adiabatic heating, and strain-rate effects.

To conduct a tensile test according to this part of ISO 6892 at 4 K, the test piece installed in a cryostat is fully submerged in liquid helium (He) and tested using displacement control at a nominal strain rate of 10‚àí3 s‚àí1 or less.

NOTE The boiling point of the rare 3He isotope is 3,2 K. Usually, the tests are performed in 4He or a mixture of 3He and 4He with a high concentration of 4He. Therefore, the temperature is, as designated before, 4 K.

Edition

1

Published Date

2015-09-29

Status

PUBLISHED

Pages

13

Language Detail Icon

English

Format Secure Icon

Secure PDF

Abstract

ISO 6892-4:2015 specifies the method of tensile testing of metallic materials in liquid helium (the boiling point is ?269 °C or 4,2 K, designated as 4 K) and defines the mechanical properties that can be determined.

This part of ISO 6892 may apply also to tensile testing at cryogenic temperatures (less than ?196 °C or 77 K), which requires special apparatus, smaller test pieces, and concern for serrated yielding, adiabatic heating, and strain-rate effects.

To conduct a tensile test according to this part of ISO 6892 at 4 K, the test piece installed in a cryostat is fully submerged in liquid helium (He) and tested using displacement control at a nominal strain rate of 10‚àí3 s‚àí1 or less.

NOTE The boiling point of the rare 3He isotope is 3,2 K. Usually, the tests are performed in 4He or a mixture of 3He and 4He with a high concentration of 4He. Therefore, the temperature is, as designated before, 4 K.