Search
×
FR

Placeholder headline

This is just a placeholder headline

API Technical Report TDB-6 Chapter 6 – Density

$

204

BUY NOW

Placeholder headline

This is just a placeholder headline

API STD 560: Fired Heaters for General Refinery Services

$

721

BUY NOW

Placeholder headline

This is just a placeholder headline

API STD 64: Diverter Equipment Systems

$

324

BUY NOW

Placeholder headline

This is just a placeholder headline

API MPMS CH 17.10.1: Refrigerated Light Hydrocarbon Fluids – Measurement of Cargoes on Board LNG Carries

$

417

BUY NOW

Placeholder headline

This is just a placeholder headline

API RP 13B-1: Testing Water-based Drilling Fluids

$

418

BUY NOW

Placeholder headline

This is just a placeholder headline

API Technical Report TDB-12 Chapter 12 – Thermal Conductivity

$

214

BUY NOW

Placeholder headline

This is just a placeholder headline

API 16FI Frac Iron Guidelines and Requirements

$

129

BUY NOW

ISO 8424:2023

ISO 8424:2023 Raw optical glass – Resistance to attack by aqueous acidic solutions – Test method and classification

CDN $173.00

SKU: 5f71e482f2c5 Categories: ,

Description

This document specifies two methods for testing the resistance of raw optical glasses to attack by aqueous acidic solutions and defines a classification of optical glasses according to the acid resistance determined by these methods.

The surface method tests the resistance of the polished plate-shaped optical glass to attack by aqueous acidic solutions at 25 °C for a specified time and indicates the class determined by this method as “SR-S”.

The powder method tests the resistance of crushed granular optical glass to attack by an acidic aqueous solution at above 98 °C for 1 h, and indicates the class determined by this method as “SR-P”.

Edition

3

Published Date

2023-07-28

Status

PUBLISHED

Pages

17

Language Detail Icon

English

Format Secure Icon

Secure PDF

Abstract

This document specifies two methods for testing the resistance of raw optical glasses to attack by aqueous acidic solutions and defines a classification of optical glasses according to the acid resistance determined by these methods.

The surface method tests the resistance of the polished plate-shaped optical glass to attack by aqueous acidic solutions at 25 °C for a specified time and indicates the class determined by this method as “SR-S”.

The powder method tests the resistance of crushed granular optical glass to attack by an acidic aqueous solution at above 98 °C for 1 h, and indicates the class determined by this method as “SR-P”.

Previous Editions

Can’t find what you are looking for?

Please contact us at: