Stress Corrosion Cracking of Corrosion Resistant Alloys in Halide Brines Exposed to Ac
Description
To understand the effects of brine compositions on the CRAs, a joint industry project was formed under the auspices of the American Petroleum Institute (API). It has been known as the CRAs in Brine Testing Program. Under its auspices, work has been underway for a number of years on understanding the interaction of brine chemistry and CRAs. The current paper evaluates the SCC risks of a range of CRAs in various halide brine compositions for the case of exposure to acidic production gas (CO2+H2S). Also evaluated are SCC risks due to air exposure. However, the testing became focused on a group of martensitic stainless steels alloyed with Ni and Mo, that are collectively referred to as modified 13Cr martensitic SS, or alternatively in some publications as super (S13Cr) martensitic SSs. Most tests evaluated the as-received brine, excluding proprietary additives such as corrosion inhibitor or oxygen scavengers. For completeness and comparison, test results provided by member companies in the
Edition
1
Published Date
2017-11-14
Status
Previous Edition
Pages
39
Format 
Secure PDF
Secure – PDF details
- Save your file locally or view it via a web viewer
- Viewing permissions are restricted exclusively to the purchaser
- Device limits - 3
- Printing – Enabled only to print (1) copy
See more about our Environmental Commitment
Abstract
To understand the effects of brine compositions on the CRAs, a joint industry project was formed under the auspices of the American Petroleum Institute (API). It has been known as the CRAs in Brine Testing Program. Under its auspices, work has been underway for a number of years on understanding the interaction of brine chemistry and CRAs. The current paper evaluates the SCC risks of a range of CRAs in various halide brine compositions for the case of exposure to acidic production gas (CO2+H2S). Also evaluated are SCC risks due to air exposure. However, the testing became focused on a group of martensitic stainless steels alloyed with Ni and Mo, that are collectively referred to as modified 13Cr martensitic SS, or alternatively in some publications as super (S13Cr) martensitic SSs. Most tests evaluated the as-received brine, excluding proprietary additives such as corrosion inhibitor or oxygen scavengers. For completeness and comparison, test results provided by member companies in the
Previous Editions
Can’t find what you are looking for?
Please contact us at:
Related Documents
-

API TR 10TR1, 2nd Edition: Cement Sheath Evaluation
CDN $312.00 Add to cart -

API RP 10G, 1st Edition: Product Evaluation, Application, and Testing of Stage Cementing Collars
CDN $277.00 Add to cart -

API RP 10B-6: Amendment
CDN $0.00 Add to cart -

API RP 100-1, 1st Edition: Hydraulic Fracturing — Well Integrity and Fracture Containment
CDN $196.00 Add to cart