ISO 11357:2013
ISO 11357:2013 Plastics – Differential scanning calorimetry (DSC) – Part 5: Determination of characteristic reaction-curve temperatures and times, enthalpy of reaction and degree of conversion
CDN $124.00
Description
ISO 11357-5:2013 specifies a method for the determination of reaction temperatures and times, enthalpies of reaction, and degrees of conversion using differential scanning calorimetry (DSC).
The method applies to monomers, prepolymers, and polymers in the solid or liquid state. The material can contain fillers and/or initiators in the solid or liquid state.
Edition
2
Published Date
2013-03-15
Status
PUBLISHED
Pages
10
Format 
Secure PDF
Secure – PDF details
- Save your file locally or view it via a web viewer
- Viewing permissions are restricted exclusively to the purchaser
- Device limits - 3
- Printing – Enabled only to print (1) copy
See more about our Environmental Commitment
Abstract
ISO 11357-5:2013 specifies a method for the determination of reaction temperatures and times, enthalpies of reaction, and degrees of conversion using differential scanning calorimetry (DSC).
The method applies to monomers, prepolymers, and polymers in the solid or liquid state. The material can contain fillers and/or initiators in the solid or liquid state.
Previous Editions
Can’t find what you are looking for?
Please contact us at:
Related Documents
-

ISO 4006:1991 Measurement of fluid flow in closed conduits – Vocabulary and symbols
CDN $391.00 Add to cart -

ISO 2382:2015 Information technology – Vocabulary
CDN $0.00 Add to cart -

ISO 80004:2011 Nanotechnologies – Vocabulary – Part 7: Diagnostics and therapeutics for healthcare
CDN $129.00 Add to cart -

ISO 80004:2021 Nanotechnologies – Vocabulary – Part 6: Nano-object characterization
CDN $85.00 Add to cart