Search
×
FR

Placeholder headline

This is just a placeholder headline

API Technical Report TDB-6 Chapter 6 – Density

$

204

BUY NOW

Placeholder headline

This is just a placeholder headline

API STD 560: Fired Heaters for General Refinery Services

$

721

BUY NOW

Placeholder headline

This is just a placeholder headline

API STD 64: Diverter Equipment Systems

$

324

BUY NOW

Placeholder headline

This is just a placeholder headline

API MPMS CH 17.10.1: Refrigerated Light Hydrocarbon Fluids – Measurement of Cargoes on Board LNG Carries

$

417

BUY NOW

Placeholder headline

This is just a placeholder headline

API RP 13B-1: Testing Water-based Drilling Fluids

$

418

BUY NOW

Placeholder headline

This is just a placeholder headline

API Technical Report TDB-12 Chapter 12 – Thermal Conductivity

$

214

BUY NOW

Placeholder headline

This is just a placeholder headline

API 16FI Frac Iron Guidelines and Requirements

$

129

BUY NOW

ISO 14270:2016

ISO 14270:2016 Resistance welding – Destructive testing of welds – Specimen dimensions and procedure for mechanized peel testing resistance spot, seam and embossed projection welds

CDN $173.00

SKU: 88dd852c6ac0 Categories: ,

Description

ISO 14270:2016 specifies specimen dimensions and a testing procedure for mechanized peel testing of single spot, seam and embossed projection welds, in overlapping sheets, in any metallic material of thickness 0,5 mm to 3 mm, where the welds have a maximum diameter of 7‚àöt (where t is the sheet thickness in mm).

For welds of diameter between 5‚àöt and 7‚àöt, the peel strength values obtained may be lower than expected when using the recommended test specimen dimensions because the test specimen width is designed for welds of diameter of 5‚àöt or less.

The object of mechanized peel testing is to determine the peel strength that the test specimen can sustain.

Edition

2

Published Date

2016-03-03

Status

PUBLISHED

Pages

17

Language Detail Icon

English

Format Secure Icon

Secure PDF

Abstract

ISO 14270:2016 specifies specimen dimensions and a testing procedure for mechanized peel testing of single spot, seam and embossed projection welds, in overlapping sheets, in any metallic material of thickness 0,5 mm to 3 mm, where the welds have a maximum diameter of 7‚àöt (where t is the sheet thickness in mm).

For welds of diameter between 5‚àöt and 7‚àöt, the peel strength values obtained may be lower than expected when using the recommended test specimen dimensions because the test specimen width is designed for welds of diameter of 5‚àöt or less.

The object of mechanized peel testing is to determine the peel strength that the test specimen can sustain.