ISO 14322:2018
ISO 14322:2018 Plastics – Epoxy resins – Determination of degree of crosslinking of crosslinked epoxy resins by differential scanning calorimetry (DSC)
CDN $115.00
Description
This document specifies a method whereby the heat of reaction generated during epoxy resin crosslinking is measured by differential scanning calorimetry (DSC). The degree of crosslinking is determined based on this result.
This method is applicable to epoxy resin systems with a moderate or slow crosslinking-reaction speed. It might not be applicable to systems with a fast crosslinking-reaction speed at ambient temperature.
Edition
2
Published Date
2018-07-19
Status
PUBLISHED
Pages
8
Format 
Secure PDF
Secure – PDF details
- Save your file locally or view it via a web viewer
- Viewing permissions are restricted exclusively to the purchaser
- Device limits - 3
- Printing – Enabled only to print (1) copy
See more about our Environmental Commitment
Abstract
This document specifies a method whereby the heat of reaction generated during epoxy resin crosslinking is measured by differential scanning calorimetry (DSC). The degree of crosslinking is determined based on this result.
This method is applicable to epoxy resin systems with a moderate or slow crosslinking-reaction speed. It might not be applicable to systems with a fast crosslinking-reaction speed at ambient temperature.
Previous Editions
Can’t find what you are looking for?
Please contact us at:
Related Documents
-

ISO 16417:2020 Earth-moving machinery – Hydraulic breakers – Terminology and commercial specifications
CDN $115.00 Add to cart -

ISO 34000:2023 Date and time – Vocabulary
CDN $76.00 Add to cart -

ISO 32210:2022 Sustainable finance – Guidance on the application of sustainability principles for organizations in the financial sector
CDN $233.00 Add to cart -

ISO 21276:2018 Clean cookstoves and clean cooking solutions – Vocabulary
CDN $76.00 Add to cart