ISO 14373:2024 Resistance welding – Procedure for spot welding of uncoated and coated low-carbon steels
CDN $173.00
Description
This document specifies requirements for resistance spot welding in the fabrication of assemblies of uncoated and metallic-coated or weldable non-metallic-coated low-carbon steel, comprising two or three sheets of metal, where the maximum single-sheet thickness of components to be welded is within the range 0,4 mm to 3,0 mm.
This document is applicable to welding of sheets of the same or unequal thickness, where the thickness ratio is less than or equal to 3:1.
Welding with the following types of equipment is within the scope of this document:
a)       pedestal welding equipment;
b)       portable welding guns;
c)        automatic welding equipment where the components are fed by robots or automatic feeding equipment;
d)       multi-spot-welding machines;
e)       robotic welding machines.
Edition
3
Published Date
2024-01-22
Status
PUBLISHED
Pages
14
Format 
Secure PDF
Secure – PDF details
- Save your file locally or view it via a web viewer
- Viewing permissions are restricted exclusively to the purchaser
- Device limits - 3
- Printing – Enabled only to print (1) copy
See more about our Environmental Commitment

Abstract
This document specifies requirements for resistance spot welding in the fabrication of assemblies of uncoated and metallic-coated or weldable non-metallic-coated low-carbon steel, comprising two or three sheets of metal, where the maximum single-sheet thickness of components to be welded is within the range 0,4 mm to 3,0 mm.
This document is applicable to welding of sheets of the same or unequal thickness, where the thickness ratio is less than or equal to 3:1.
Welding with the following types of equipment is within the scope of this document:
a)       pedestal welding equipment;
b)       portable welding guns;
c)        automatic welding equipment where the components are fed by robots or automatic feeding equipment;
d)       multi-spot-welding machines;
e)       robotic welding machines.
Previous Editions
Can’t find what you are looking for?
Please contact us at:
Related Documents
-
ISO 80004:2021 Nanotechnologies – Vocabulary – Part 6: Nano-object characterization
0 out of 5CDN $76.00 Add to cart -
ISO 3833:1977 Road vehicles – Types – Terms and definitions
0 out of 5CDN $115.00 Add to cart -
ISO 8927:1991 Earth-moving machinery – Machine availability – Vocabulary
0 out of 5CDN $233.00 Add to cart -
ISO 5078:2025 Management of terminology resources – Terminology extraction
0 out of 5CDN $233.00 Add to cart