ISO 15610:2024
ISO 15610:2024 Specification and qualification of welding procedures for metallic materials – Qualification based on tested welding consumables
CDN $85.00
Description
This document specifies how a welding procedure can be qualified by using tested welding consumable data. It expands on the requirements given in ISO 15607.
In addition, it gives the range of qualification.
Application of this document is limited to parent material groups 1.1, 8.1, 21, 22.1 and 22.2 in accordance with ISO/TR 15608, which produce acceptable microstructures and properties in the heat-affected zone which do not deteriorate significantly in service.
This document is limited to:
–¬†¬†¬†¬† butt welds and fillet welds in material of thicknesses t¬†‚⧬†40¬†mm (groups 1.1 and 8.1) and t¬†‚⧬†20¬†mm (groups 21, 22.1 and 22.2);
–¬†¬†¬†¬† fillet welds with throat thickness a¬†‚╬†1¬†mm.
This document is not applicable when any of the following is specified for the welded joint:
a)       hardness;
b)       impact properties;
c)        preheating;
d)       controlled heat input;
e)       interpass temperature;
f)         post-weld heat treatment.
The use of this document can also be restricted by an application standard, specification or other documents.
Edition
3
Published Date
2024-03-06
Status
PUBLISHED
Pages
6
Format 
Secure PDF
Secure – PDF details
- Save your file locally or view it via a web viewer
- Viewing permissions are restricted exclusively to the purchaser
- Device limits - 3
- Printing – Enabled only to print (1) copy
See more about our Environmental Commitment
Abstract
This document specifies how a welding procedure can be qualified by using tested welding consumable data. It expands on the requirements given in ISO 15607.
In addition, it gives the range of qualification.
Application of this document is limited to parent material groups 1.1, 8.1, 21, 22.1 and 22.2 in accordance with ISO/TR 15608, which produce acceptable microstructures and properties in the heat-affected zone which do not deteriorate significantly in service.
This document is limited to:
-     butt welds and fillet welds in material of thicknesses t ≤ 40 mm (groups 1.1 and 8.1) and t ≤ 20 mm (groups 21, 22.1 and 22.2);
-     fillet welds with throat thickness a ≥ 1 mm.
This document is not applicable when any of the following is specified for the welded joint:
a)       hardness;
b)       impact properties;
c)        preheating;
d)       controlled heat input;
e)       interpass temperature;
f)         post-weld heat treatment.
The use of this document can also be restricted by an application standard, specification or other documents.
Previous Editions
Can’t find what you are looking for?
Please contact us at:
Related Documents
-

ISO 25901:2022 Welding and allied processes – Vocabulary – Part 2: Health and safety
CDN $85.00 Add to cart -

ISO 15011:2017 Health and safety in welding and allied processes – Laboratory method for sampling fume and gases – Part 4: Fume data sheets
CDN $259.00 Add to cart -

ISO 25980:2023 Health and safety in welding and allied processes – Transparent welding curtains, strips and screens for arc welding processes
CDN $192.00 Add to cart -

ISO 13920:2023 Welding – General tolerances for welded constructions – Dimensions for lengths and angles, shape and position
CDN $129.00 Add to cart