ISO 15612:2018
ISO 15612:2018 Specification and qualification of welding procedures for metallic materials – Qualification by adoption of a standard welding procedure specification
CDN $76.00
Description
This document:
– specifies how a user can follow a standard welding procedure specification (SWPS) based on welding procedure qualification tests performed by a different organization;
– specifies the range for the use of SWPSs in accordance with ISO 15607;
– specifies the requirements for qualification of welding procedures to be issued as SWPSs; and
– specifies the requirements for organizations adopting SWPSs.
The use of this document can be restricted by an application standard or a specification.
This document is applicable to welding of steels and aluminium and its alloys (see 4.1).
All new standard welding procedure qualifications are to be carried out in accordance with this document from the date of its issue. However, this document does not invalidate previous standard welding procedure qualifications made to former standards, specifications or previous editions of this document
Edition
2
Published Date
2018-06-18
Status
PUBLISHED
Pages
5
Format 
Secure PDF
Secure – PDF details
- Save your file locally or view it via a web viewer
- Viewing permissions are restricted exclusively to the purchaser
- Device limits - 3
- Printing – Enabled only to print (1) copy
See more about our Environmental Commitment
Abstract
This document:
- specifies how a user can follow a standard welding procedure specification (SWPS) based on welding procedure qualification tests performed by a different organization;
- specifies the range for the use of SWPSs in accordance with ISO 15607;
- specifies the requirements for qualification of welding procedures to be issued as SWPSs; and
- specifies the requirements for organizations adopting SWPSs.
The use of this document can be restricted by an application standard or a specification.
This document is applicable to welding of steels and aluminium and its alloys (see 4.1).
All new standard welding procedure qualifications are to be carried out in accordance with this document from the date of its issue. However, this document does not invalidate previous standard welding procedure qualifications made to former standards, specifications or previous editions of this document
Previous Editions
Can’t find what you are looking for?
Please contact us at:
Related Documents
-

ISO 13469:2014 Mechanical joining – Form-fit blind rivets and (lock) bolt joints – Specifications and qualification of testing procedures
CDN $173.00 Add to cart -

ISO 17658:2002 Welding – Imperfections in oxyfuel flame cuts, laser beam cuts and plasma cuts – Terminology
CDN $173.00 Add to cart -

ISO 25901:2016 Welding and allied processes – Vocabulary – Part 3: Welding processes
CDN $76.00 Add to cart -

ISO 17677:2021 Resistance welding – Vocabulary – Part 1: Spot, projection and seam welding
CDN $76.00 Add to cart