This document specifies how a preliminary welding procedure specification (pWPS) is qualified by welding procedure tests.
This document defines the conditions for the execution of welding procedure tests and the range of qualification for welding procedures for all welding operations within the qualification of this document.
Two classes of welding procedure tests are given in order to permit application to a wide range of welded fabrication. They are designated by classes A and B. In class A, the extent of testing is greater and the ranges of qualification are more restrictive than in class B.
Procedure tests carried out to class A automatically qualify for class B requirements, but not vice-versa.
When no class is specified in a contract or application standard, all the requirements of class A apply.
NOTE         Class B corresponds to level 1 and class A corresponds to level 2 in accordance with ISO 15614-1.
This document applies to upset (resistance butt) welding and flash welding of any metallic materials in all product forms (e.g. with solid, tubular, flat or circular cross-sections). It covers the following resistance welding processes, as defined in ISO 4063:2023:
–    24 – flash welding, using direct current or alternating current with various movement sequences, constant flashing and pulsed flashing;
–    25 – resistance butt welding (upset welding), using direct current or alternating current with various current and pressure sequences.
Edition
4
Published Date
2023-11-13
Status
PUBLISHED
Pages
13
Format 
Secure PDF
Secure – PDF details
- Save your file locally or view it via a web viewer
- Viewing permissions are restricted exclusively to the purchaser
- Device limits - 3
- Printing – Enabled only to print (1) copy
See more about our Environmental Commitment

Abstract
This document specifies how a preliminary welding procedure specification (pWPS) is qualified by welding procedure tests.
This document defines the conditions for the execution of welding procedure tests and the range of qualification for welding procedures for all welding operations within the qualification of this document.
Two classes of welding procedure tests are given in order to permit application to a wide range of welded fabrication. They are designated by classes A and B. In class A, the extent of testing is greater and the ranges of qualification are more restrictive than in class B.
Procedure tests carried out to class A automatically qualify for class B requirements, but not vice-versa.
When no class is specified in a contract or application standard, all the requirements of class A apply.
NOTE         Class B corresponds to level 1 and class A corresponds to level 2 in accordance with ISO 15614-1.
This document applies to upset (resistance butt) welding and flash welding of any metallic materials in all product forms (e.g. with solid, tubular, flat or circular cross-sections). It covers the following resistance welding processes, as defined in ISO 4063:2023:
-    24 – flash welding, using direct current or alternating current with various movement sequences, constant flashing and pulsed flashing;
-    25 – resistance butt welding (upset welding), using direct current or alternating current with various current and pressure sequences.
Previous Editions
Can’t find what you are looking for?
Please contact us at:
Related Documents
-
ISO 20674:2019 Information and documentation – Transliteration of scripts in use in Thailand – Part 1: Transliteration of Akson-Thai-Noi
0 out of 5CDN $173.00 Add to cart -
ISO 1176:1990 Road vehicles – Masses – Vocabulary and codes
0 out of 5CDN $115.00 Add to cart -
ISO 3833:1977 Road vehicles – Types – Terms and definitions
0 out of 5CDN $115.00 Add to cart -
ISO 21636:2024 Language coding – A framework for language varieties – Part 1: Vocabulary
0 out of 5CDN $173.00 Add to cart