ISO 15614:2008
ISO 15614:2008 Specification and qualification of welding procedures for metallic materials – Welding procedure test – Part 3: Fusion welding of non-alloyed and low-alloyed cast irons
CDN $173.00
Description
ISO 15614-3:2008 specifies how a preliminary welding procedure specification (pWPS) for production and repair welding of non-alloyed and low-alloyed cast irons is qualified by fusion welding procedure tests.
ISO 15614-3:2008 defines the conditions for execution of the welding procedure tests and the range of qualification for welding procedures for all practical welding operations within the range of a defined list of variables.
ISO 15614-3:2008 is applicable to all new welding procedures. However, it does not invalidate previous welding procedure tests made to former national standards or specifications. Where additional tests have to be carried out to make the qualification technically equivalent, it is only necessary to do the additional tests on a test piece made in accordance with ISO 15614-3:2008.
Additional tests may be required by application standards.
ISO 15614-3:2008 is applicable to welding non-alloyed and low-alloyed grey cast iron castings according to: EN 1561; EN 1562; EN 1563; and EN 1564.
The principles of ISO 15614-3:2008 are also applicable for welding cast iron to steel or to other unalloyed and low-alloyed cast iron materials.
Edition
1
Published Date
2008-03-04
Status
PUBLISHED
Pages
17
Format 
Secure PDF
Secure – PDF details
- Save your file locally or view it via a web viewer
- Viewing permissions are restricted exclusively to the purchaser
- Device limits - 3
- Printing – Enabled only to print (1) copy
See more about our Environmental Commitment
Abstract
ISO 15614-3:2008 specifies how a preliminary welding procedure specification (pWPS) for production and repair welding of non-alloyed and low-alloyed cast irons is qualified by fusion welding procedure tests.
ISO 15614-3:2008 defines the conditions for execution of the welding procedure tests and the range of qualification for welding procedures for all practical welding operations within the range of a defined list of variables.
ISO 15614-3:2008 is applicable to all new welding procedures. However, it does not invalidate previous welding procedure tests made to former national standards or specifications. Where additional tests have to be carried out to make the qualification technically equivalent, it is only necessary to do the additional tests on a test piece made in accordance with ISO 15614-3:2008.
Additional tests may be required by application standards.
ISO 15614-3:2008 is applicable to welding non-alloyed and low-alloyed grey cast iron castings according to: EN 1561; EN 1562; EN 1563; and EN 1564.
The principles of ISO 15614-3:2008 are also applicable for welding cast iron to steel or to other unalloyed and low-alloyed cast iron materials.
Previous Editions
Can’t find what you are looking for?
Please contact us at:
Related Documents
-

ISO 15011:2012 Health and safety in welding and allied processes – Laboratory method for sampling fume and gases – Part 6: Procedure for quantitative determination of fume and gases from resistance spot welding
CDN $233.00 Add to cart -

ISO 15607:2019 Specification and qualification of welding procedures for metallic materials – General rules
CDN $115.00 Add to cart -

ISO 9692:2024 Welding and allied processes – Joint preparation – Part 2: Submerged arc welding of steels
CDN $115.00 Add to cart -

ISO 17658:2002 Welding – Imperfections in oxyfuel flame cuts, laser beam cuts and plasma cuts – Terminology
CDN $173.00 Add to cart