Search
×
FR

Placeholder headline

This is just a placeholder headline

API Technical Report TDB-6 Chapter 6 – Density

$

204

BUY NOW

Placeholder headline

This is just a placeholder headline

API STD 560: Fired Heaters for General Refinery Services

$

721

BUY NOW

Placeholder headline

This is just a placeholder headline

API STD 64: Diverter Equipment Systems

$

324

BUY NOW

Placeholder headline

This is just a placeholder headline

API MPMS CH 17.10.1: Refrigerated Light Hydrocarbon Fluids – Measurement of Cargoes on Board LNG Carries

$

417

BUY NOW

Placeholder headline

This is just a placeholder headline

API RP 13B-1: Testing Water-based Drilling Fluids

$

418

BUY NOW

Placeholder headline

This is just a placeholder headline

API Technical Report TDB-12 Chapter 12 – Thermal Conductivity

$

214

BUY NOW

Placeholder headline

This is just a placeholder headline

API 16FI Frac Iron Guidelines and Requirements

$

129

BUY NOW

ISO 16432:2006

ISO 16432:2006 Resistance welding – Procedure for projection welding of uncoated and coated low carbon steels using embossed projection(s)

CDN $173.00

SKU: 40f2224dda1d Categories: ,

Description

ISO 16432:2006 specifies requirements for embossed-resistance-projection welding in the fabrication of assemblies of uncoated and metallic coated low carbon steel comprising two thicknesses of metal, where the maximum single sheet thickness of components to be welded is within the range 0,4 mm to 3 mm for the following materials:

  • uncoated steels;
  • hot-dip zinc or iron-zinc alloy (galvannealed) coated steel;
  • electrolytic zinc, zinc-iron, or zinc-nickel coated steel;
  • aluminium coated steel;
  • zinc-aluminium coated steel.

Organic coated or primer coated steels are not covered by ISO 16432:2006.

Edition

1

Published Date

2006-02-03

Status

PUBLISHED

Pages

15

Language Detail Icon

English

Format Secure Icon

Secure PDF

Abstract

ISO 16432:2006 specifies requirements for embossed-resistance-projection welding in the fabrication of assemblies of uncoated and metallic coated low carbon steel comprising two thicknesses of metal, where the maximum single sheet thickness of components to be welded is within the range 0,4 mm to 3 mm for the following materials:

  • uncoated steels;
  • hot-dip zinc or iron-zinc alloy (galvannealed) coated steel;
  • electrolytic zinc, zinc-iron, or zinc-nickel coated steel;
  • aluminium coated steel;
  • zinc-aluminium coated steel.

Organic coated or primer coated steels are not covered by ISO 16432:2006.

Previous Editions

Can’t find what you are looking for?

Please contact us at: