“ISO 18211:2016 Non-destructive testing – Long-range inspection of above-ground pipelines and plant piping using guided wave testing with axial propagation” has been added to your cart. View cart

ISO 16433:2006
ISO 16433:2006 Resistance welding – Procedure for seam welding of uncoated and coated low carbon steels
CDN $233.00
SKU: 1d4a2527158d
Categories: ICS:25.160.10, LOGO:IIW
Description
ISO16433:2006 specifies requirements for resistance seam welding in the fabrication of assemblies of uncoated and metallic coated low carbon steel comprising two sheets of metal, where the maximum single sheet thickness of components to be welded is within the range 0,4 mm to 3 mm for the following materials:
- uncoated steels;
- hot-dip zinc or iron-zinc alloy (galvannealed) coated steel;
- electrolytic zinc, zinc-iron, or zinc-nickel coated steel;
- aluminium coated steel;
- zinc-aluminium coated steel.
Edition
1
Published Date
2006-03-29
Status
PUBLISHED
Pages
20
Format 
Secure PDF
Secure – PDF details
- Save your file locally or view it via a web viewer
- Viewing permissions are restricted exclusively to the purchaser
- Device limits - 3
- Printing – Enabled only to print (1) copy
See more about our Environmental Commitment

Abstract
ISO16433:2006 specifies requirements for resistance seam welding in the fabrication of assemblies of uncoated and metallic coated low carbon steel comprising two sheets of metal, where the maximum single sheet thickness of components to be welded is within the range 0,4 mm to 3 mm for the following materials:
- uncoated steels;
- hot-dip zinc or iron-zinc alloy (galvannealed) coated steel;
- electrolytic zinc, zinc-iron, or zinc-nickel coated steel;
- aluminium coated steel;
- zinc-aluminium coated steel.
Previous Editions
Can’t find what you are looking for?
Please contact us at:
Related Documents
-
ISO 22688:2020 Brazing – Quality requirements for brazing of metallic materials
0 out of 5CDN $273.00 Add to cart -
ISO 25239:2020 Friction stir welding – Aluminium – Part 4: Specification and qualification of welding procedures
0 out of 5CDN $233.00 Add to cart -
ISO 19675:2017 Non-destructive testing – Ultrasonic testing – Specification for a calibration block for phased array testing (PAUT)