Search
×
FR

Placeholder headline

This is just a placeholder headline

API Technical Report TDB-6 Chapter 6 – Density

$

204

BUY NOW

Placeholder headline

This is just a placeholder headline

API STD 560: Fired Heaters for General Refinery Services

$

721

BUY NOW

Placeholder headline

This is just a placeholder headline

API STD 64: Diverter Equipment Systems

$

324

BUY NOW

Placeholder headline

This is just a placeholder headline

API MPMS CH 17.10.1: Refrigerated Light Hydrocarbon Fluids – Measurement of Cargoes on Board LNG Carries

$

417

BUY NOW

Placeholder headline

This is just a placeholder headline

API RP 13B-1: Testing Water-based Drilling Fluids

$

418

BUY NOW

Placeholder headline

This is just a placeholder headline

API Technical Report TDB-12 Chapter 12 – Thermal Conductivity

$

214

BUY NOW

Placeholder headline

This is just a placeholder headline

API 16FI Frac Iron Guidelines and Requirements

$

129

BUY NOW

ISO 16540:2015

ISO 16540:2015 Corrosion of metals and alloys – Methodology for determining the resistance of metals to stress corrosion cracking using the four-point bend method

CDN $173.00

Description

ISO 16540:2015 provides guidelines for the use of four-point bend testing to evaluate the resistance of metals including carbon steel, low alloy steels, and corrosion resistant alloys (CRAs) to stress corrosion cracking. The method gives guidance on testing of both parent plate and welds and includes procedures for metals that have no distinct yield point in their stress-strain behaviour as well as metals with a distinct yield point. The emphasis in this International Standard is on the generic methodology of the four-point bend test. Service application will be varied and the relevant industry standard is to be consulted where appropriate.

Edition

1

Published Date

2015-09-29

Status

PUBLISHED

Pages

18

Language Detail Icon

English

Format Secure Icon

Secure PDF

Abstract

ISO 16540:2015 provides guidelines for the use of four-point bend testing to evaluate the resistance of metals including carbon steel, low alloy steels, and corrosion resistant alloys (CRAs) to stress corrosion cracking. The method gives guidance on testing of both parent plate and welds and includes procedures for metals that have no distinct yield point in their stress-strain behaviour as well as metals with a distinct yield point. The emphasis in this International Standard is on the generic methodology of the four-point bend test. Service application will be varied and the relevant industry standard is to be consulted where appropriate.