ISO 19399:2016

ISO 19399:2016 Paints and varnishes – Wedge-cut method for determination of film thickness (scribe and drill method)

CDN $310.00

SKU: 0363099806f6 Category:

Description

ISO 19399:2016 specifies a destructive method for determination of the dry film thickness, in which damage to the coat caused in a definite manner is evaluated microscopically. The method is suitable for almost all coat-substrate combinations and also allows determination of the single film thicknesses of coating systems.

The method cannot be applied or can only be applied with restrictions in case of

– too soft and/or elastic coatings (no recognizable scribe or drill hole can be observed),

– hard (cannot be scribed/drilled) or too soft and/or elastic substrates,

– too low visual contrast between the coating and substrate, and

– film thicknesses that are larger than the depth of field of the measuring microscope.

Edition

1

Published Date

2016-04-26

Status

PUBLISHED

Pages

27

Language Detail Icon

English

Format Secure Icon

Secure PDF

Abstract

ISO 19399:2016 specifies a destructive method for determination of the dry film thickness, in which damage to the coat caused in a definite manner is evaluated microscopically. The method is suitable for almost all coat-substrate combinations and also allows determination of the single film thicknesses of coating systems.

The method cannot be applied or can only be applied with restrictions in case of

- too soft and/or elastic coatings (no recognizable scribe or drill hole can be observed),

- hard (cannot be scribed/drilled) or too soft and/or elastic substrates,

- too low visual contrast between the coating and substrate, and

- film thicknesses that are larger than the depth of field of the measuring microscope.