ISO 204:2023
ISO 204:2023 Metallic materials – Uniaxial creep testing in tension – Method of test
CDN $312.00
Description
This document specifies the methods for:
a)    uninterrupted creep tests with continuous monitoring of extension;
b)    interrupted creep tests with periodic measurement of elongation;
c)    stress rupture tests where normally only the time to fracture is measured;
d)    a test to verify that a predetermined time can be exceeded under a given force, with the elongation or extension not necessarily being reported.
NOTE       A creep test can be continued until fracture has occurred or it can be stopped before fracture.
Edition
4
Published Date
2023-07-25
Status
PUBLISHED
Pages
48
Format 
Secure PDF
Secure – PDF details
- Save your file locally or view it via a web viewer
- Viewing permissions are restricted exclusively to the purchaser
- Device limits - 3
- Printing – Enabled only to print (1) copy
See more about our Environmental Commitment
Abstract
This document specifies the methods for:
a)    uninterrupted creep tests with continuous monitoring of extension;
b)    interrupted creep tests with periodic measurement of elongation;
c)    stress rupture tests where normally only the time to fracture is measured;
d)    a test to verify that a predetermined time can be exceeded under a given force, with the elongation or extension not necessarily being reported.
NOTE       A creep test can be continued until fracture has occurred or it can be stopped before fracture.
Previous Editions
Can’t find what you are looking for?
Please contact us at:
Related Documents
-

ISO 2740:2023 Sintered metal materials, excluding hardmetals – Tensile test pieces
CDN $115.00 Add to cart -

ISO 28079:2009 Hardmetals – Palmqvist toughness test
CDN $115.00 Add to cart -

ISO 14317:2015 Sintered metal materials excluding hardmetals – Determination of compressive yield strength
CDN $76.00 Add to cart -

ISO 3325:2001 Sintered metal materials, excluding hardmetals – Determination of transverse rupture strength – Amendment 1: Precision statement
CDN $32.00 Add to cart