ISO 2062:2009
ISO 2062:2009 Textiles – Yarns from packages – Determination of single-end breaking force and elongation at break using constant rate of extension (CRE) tester
CDN $131.00
Description
ISO 2062:2009 specifies methods for the determination of the breaking force and elongation at break of textile yarns taken from packages.
Four methods are given:
- A: manual; specimens are taken directly from conditioned packages;
- B: automatic; specimens are taken directly from conditioned packages;
- C: manual; relaxed test skeins are used after conditioning;
- D: manual; specimens are used after wetting.
Method C is used in cases of dispute regarding elongation at break of the yarn.
ISO 2062:2009 specifies methods using constant rate of specimen extension (CRE) tensile testers. Testing on the now obsolete constant rate of travel (CRT) and constant rate of loading (CRL) instruments is covered, for information, in Annex A, in recognition of the fact that these instruments are still in use and can be used by agreement.
ISO 2062:2009 applies to all types of yarns, except glass, elastomeric, aramid, high molecular polyethylene (HMPE), ultra high molecular polyethylene (UHMPE), ceramic and carbon yarns and polyolefin tape.
ISO 2062:2009 is applicable to yarns from packages but can be applied to yarns extracted from fabrics, subject to agreement between the interested parties.
ISO 2062:2009 is intended for the single-end (single-strand) testing of yarns.
Edition
3
Published Date
2009-11-26
Status
PUBLISHED
Pages
10
Format 
Secure PDF
Secure – PDF details
- Save your file locally or view it via a web viewer
- Viewing permissions are restricted exclusively to the purchaser
- Device limits - 3
- Printing – Enabled only to print (1) copy
See more about our Environmental Commitment
Abstract
ISO 2062:2009 specifies methods for the determination of the breaking force and elongation at break of textile yarns taken from packages.
Four methods are given:
- A: manual; specimens are taken directly from conditioned packages;
- B: automatic; specimens are taken directly from conditioned packages;
- C: manual; relaxed test skeins are used after conditioning;
- D: manual; specimens are used after wetting.
Method C is used in cases of dispute regarding elongation at break of the yarn.
ISO 2062:2009 specifies methods using constant rate of specimen extension (CRE) tensile testers. Testing on the now obsolete constant rate of travel (CRT) and constant rate of loading (CRL) instruments is covered, for information, in Annex A, in recognition of the fact that these instruments are still in use and can be used by agreement.
ISO 2062:2009 applies to all types of yarns, except glass, elastomeric, aramid, high molecular polyethylene (HMPE), ultra high molecular polyethylene (UHMPE), ceramic and carbon yarns and polyolefin tape.
ISO 2062:2009 is applicable to yarns from packages but can be applied to yarns extracted from fabrics, subject to agreement between the interested parties.
ISO 2062:2009 is intended for the single-end (single-strand) testing of yarns.
Previous Editions
Can’t find what you are looking for?
Please contact us at:
Related Documents
-

ISO 23733:2007 Textiles – Chenille yarns – Test method for the determination of linear density
CDN $131.00 Add to cart -

ISO 18067:2015 Textiles – Synthetic filament yarns – Determination of shrinkage in dry-hot air (after treatment)
CDN $131.00 Add to cart -

ISO 1139:1973 Textiles – Designation of yarns
CDN $82.00 Add to cart -

ISO 8160:1987 Textiles – Textured filament yarns – Vocabulary
CDN $86.00 Add to cart