Search
×
FR

Placeholder headline

This is just a placeholder headline

API Technical Report TDB-6 Chapter 6 – Density

$

204

BUY NOW

Placeholder headline

This is just a placeholder headline

API STD 560: Fired Heaters for General Refinery Services

$

721

BUY NOW

Placeholder headline

This is just a placeholder headline

API STD 64: Diverter Equipment Systems

$

324

BUY NOW

Placeholder headline

This is just a placeholder headline

API MPMS CH 17.10.1: Refrigerated Light Hydrocarbon Fluids – Measurement of Cargoes on Board LNG Carries

$

417

BUY NOW

Placeholder headline

This is just a placeholder headline

API RP 13B-1: Testing Water-based Drilling Fluids

$

418

BUY NOW

Placeholder headline

This is just a placeholder headline

API Technical Report TDB-12 Chapter 12 – Thermal Conductivity

$

214

BUY NOW

Placeholder headline

This is just a placeholder headline

API 16FI Frac Iron Guidelines and Requirements

$

129

BUY NOW

ISO 21022:2018

ISO 21022:2018 Test method for fibre-reinforced cementitious composites – Load-deflection curve using circular plates

CDN $173.00

SKU: 3c43d7e108c0 Categories: , ,

Description

This document specifies a test method for evaluating flexural performance of fibre-reinforced cementitious composites (FRCCs) using derived parameters. These parameters are derived from the load-deflection curve obtained by testing a circular specimen supported on a concentric ring and loaded by another ring with a smaller diameter. The performance of FRCCs tested by this method is characterized for biaxial properties.

This test method provides for the determination of first-cracking load and the corresponding stress. It also provides for the determination of specimen toughness based on the area under the load-deflection curve up to the deflections at the first-cracking and peak loads. For determining the toughness value, this test method is intended primarily for use with FRCCs that exhibit deflection hardening behaviour. This test method is not intended for materials that exhibit deflection-softening behaviour.

Edition

1

Published Date

2018-11-27

Status

PUBLISHED

Pages

13

Language Detail Icon

English

Format Secure Icon

Secure PDF

Abstract

This document specifies a test method for evaluating flexural performance of fibre-reinforced cementitious composites (FRCCs) using derived parameters. These parameters are derived from the load-deflection curve obtained by testing a circular specimen supported on a concentric ring and loaded by another ring with a smaller diameter. The performance of FRCCs tested by this method is characterized for biaxial properties.

This test method provides for the determination of first-cracking load and the corresponding stress. It also provides for the determination of specimen toughness based on the area under the load-deflection curve up to the deflections at the first-cracking and peak loads. For determining the toughness value, this test method is intended primarily for use with FRCCs that exhibit deflection hardening behaviour. This test method is not intended for materials that exhibit deflection-softening behaviour.