ISO 22848:2021
ISO 22848:2021 Corrosion of metals and alloys – Test method for measuring the stress corrosion crack growth rate of steels and alloys under static-load conditions in high-temperature water
CDN $259.00
Description
This document specifies a test method for determining the stress corrosion crack (SCC) growth rate of steels and alloys under static-load conditions in high-temperature water, such as the simulated water environment of light water reactors. The crack length of the specimen is monitored by a potential drop method (PDM) during the test in an autoclave.
The test method is applicable to stainless steels, nickel base alloys, low alloy steels, carbon steels and other alloys.
Edition
1
Published Date
2021-02-19
Status
PUBLISHED
Pages
25
Format 
Secure PDF
Secure – PDF details
- Save your file locally or view it via a web viewer
- Viewing permissions are restricted exclusively to the purchaser
- Device limits - 3
- Printing – Enabled only to print (1) copy
See more about our Environmental Commitment
Abstract
This document specifies a test method for determining the stress corrosion crack (SCC) growth rate of steels and alloys under static-load conditions in high-temperature water, such as the simulated water environment of light water reactors. The crack length of the specimen is monitored by a potential drop method (PDM) during the test in an autoclave.
The test method is applicable to stainless steels, nickel base alloys, low alloy steels, carbon steels and other alloys.
Previous Editions
Can’t find what you are looking for?
Please contact us at:
Related Documents
-

ISO 11844:2020 Corrosion of metals and alloys – Classification of low corrosivity of indoor atmospheres – Part 3: Measurement of environmental parameters affecting indoor corrosivity
CDN $129.00 Add to cart -

ISO 17475:2005 Corrosion of metals and alloys – Electrochemical test methods – Guidelines for conducting potentiostatic and potentiodynamic polarization measurements
CDN $192.00 Add to cart -

ISO 4680:2022 Corrosion of metals and alloys – Uniaxial constant-load test method for evaluating susceptibility of metals and alloys to stress corrosion cracking in high-purity water at high temperatures
CDN $305.00 Add to cart -

ISO 17081:2014 Method of measurement of hydrogen permeation and determination of hydrogen uptake and transport in metals by an electrochemical technique
CDN $259.00 Add to cart