Search
×
FR

Placeholder headline

This is just a placeholder headline

API Technical Report TDB-6 Chapter 6 – Density

$

204

BUY NOW

Placeholder headline

This is just a placeholder headline

API STD 560: Fired Heaters for General Refinery Services

$

721

BUY NOW

Placeholder headline

This is just a placeholder headline

API STD 64: Diverter Equipment Systems

$

324

BUY NOW

Placeholder headline

This is just a placeholder headline

API MPMS CH 17.10.1: Refrigerated Light Hydrocarbon Fluids – Measurement of Cargoes on Board LNG Carries

$

417

BUY NOW

Placeholder headline

This is just a placeholder headline

API RP 13B-1: Testing Water-based Drilling Fluids

$

418

BUY NOW

Placeholder headline

This is just a placeholder headline

API Technical Report TDB-12 Chapter 12 – Thermal Conductivity

$

214

BUY NOW

Placeholder headline

This is just a placeholder headline

API 16FI Frac Iron Guidelines and Requirements

$

129

BUY NOW

ISO 2376:2019

ISO 2376:2019 Anodizing of aluminium and its alloys – Determination of breakdown voltage and withstand voltage

CDN $76.00

Description

This document specifies test methods for the determination of the breakdown voltage and withstand voltage of anodic oxidation coatings on aluminium and its alloys, on flat or near-flat surfaces and on round wire. The methods are applicable to anodic oxidation coatings used primarily as electrical insulators.

The methods are not applicable to coatings in the vicinity of cut edges, the edges of holes, or sharp changes of angle on, for example, extruded shapes.

NOTE 1 Breakdown voltage and withstand voltage are affected by relative humidity.

NOTE 2 The methods described do not give satisfactory results for unsealed coatings because they are affected by the humidity in particular.

Edition

3

Published Date

2019-03-06

Status

PUBLISHED

Pages

4

Language Detail Icon

English

Format Secure Icon

Secure PDF

Abstract

This document specifies test methods for the determination of the breakdown voltage and withstand voltage of anodic oxidation coatings on aluminium and its alloys, on flat or near-flat surfaces and on round wire. The methods are applicable to anodic oxidation coatings used primarily as electrical insulators.

The methods are not applicable to coatings in the vicinity of cut edges, the edges of holes, or sharp changes of angle on, for example, extruded shapes.

NOTE 1 Breakdown voltage and withstand voltage are affected by relative humidity.

NOTE 2 The methods described do not give satisfactory results for unsealed coatings because they are affected by the humidity in particular.