REGISTER

FR
Search
×
FR

Placeholder headline

This is just a placeholder headline

API SPEC 14L: Lock Mandrels and Landing Nipples : Reaffirmed

$

273

BUY NOW

Placeholder headline

This is just a placeholder headline

API SPEC 20F: Corrosion Resistant Bolting for Use in the Petroleum and Natural Gas Industries : Reaffirmed

$

169

BUY NOW

Placeholder headline

This is just a placeholder headline

API TR 5NCL Nickel Content Limits for API 5CT Sour Service Products

$

149

BUY NOW

Placeholder headline

This is just a placeholder headline

API SPEC 19ICD: Inflow Control Devices : Reaffirmed

$

189

BUY NOW

Placeholder headline

This is just a placeholder headline

API MPMS CH 23.2: Reconciliation of Liquid Tank Car(s) Quantities : Reaffirmed

$

218

BUY NOW

Placeholder headline

This is just a placeholder headline

API SPEC 16A: Specification for Drill-through Equipment

$

322

BUY NOW

Placeholder headline

This is just a placeholder headline

API RP 13B-2: Field Testing Oil-based Drilling Fluids wA1

$

388

BUY NOW

ISO 2376:2019

ISO 2376:2019 Anodizing of aluminium and its alloys – Determination of breakdown voltage and withstand voltage

CDN $76.00

Description

This document specifies test methods for the determination of the breakdown voltage and withstand voltage of anodic oxidation coatings on aluminium and its alloys, on flat or near-flat surfaces and on round wire. The methods are applicable to anodic oxidation coatings used primarily as electrical insulators.

The methods are not applicable to coatings in the vicinity of cut edges, the edges of holes, or sharp changes of angle on, for example, extruded shapes.

NOTE 1 Breakdown voltage and withstand voltage are affected by relative humidity.

NOTE 2 The methods described do not give satisfactory results for unsealed coatings because they are affected by the humidity in particular.

Edition

3

Published Date

2019-03-06

Status

PUBLISHED

Pages

4

Language Detail Icon

English

Format Secure Icon

Secure PDF

Abstract

This document specifies test methods for the determination of the breakdown voltage and withstand voltage of anodic oxidation coatings on aluminium and its alloys, on flat or near-flat surfaces and on round wire. The methods are applicable to anodic oxidation coatings used primarily as electrical insulators.

The methods are not applicable to coatings in the vicinity of cut edges, the edges of holes, or sharp changes of angle on, for example, extruded shapes.

NOTE 1 Breakdown voltage and withstand voltage are affected by relative humidity.

NOTE 2 The methods described do not give satisfactory results for unsealed coatings because they are affected by the humidity in particular.