ISO 4680:2022
ISO 4680:2022 Corrosion of metals and alloys – Uniaxial constant-load test method for evaluating susceptibility of metals and alloys to stress corrosion cracking in high-purity water at high temperatures
CDN $273.00
Description
The document specifies a method for undertaking uniaxial constant load testing of the susceptibility of a metal, or an alloy, to stress corrosion cracking (SCC) in high-purity water environments at high temperature (above the boiling point of water at normal pressures) and pressure. The test method is particularly applicable to simulated primary water environments of light water reactors (LWRs).
The test method enables assessment of the relative resistance to SCC of a material in different environments and the comparative resistance of different materials (using the same environment, specimen dimensions and loading).
The terms “metal” and “alloy”, as used in the document, include weld metals and weld heat affected zones.
Edition
1
Published Date
2022-12-19
Status
PUBLISHED
Pages
27
Format 
Secure PDF
Secure – PDF details
- Save your file locally or view it via a web viewer
- Viewing permissions are restricted exclusively to the purchaser
- Device limits - 3
- Printing – Enabled only to print (1) copy
See more about our Environmental Commitment
Abstract
The document specifies a method for undertaking uniaxial constant load testing of the susceptibility of a metal, or an alloy, to stress corrosion cracking (SCC) in high-purity water environments at high temperature (above the boiling point of water at normal pressures) and pressure. The test method is particularly applicable to simulated primary water environments of light water reactors (LWRs).
The test method enables assessment of the relative resistance to SCC of a material in different environments and the comparative resistance of different materials (using the same environment, specimen dimensions and loading).
The terms “metal” and “alloy”, as used in the document, include weld metals and weld heat affected zones.
Previous Editions
Can’t find what you are looking for?
Please contact us at:
Related Documents
-

ISO 16417:2020 Earth-moving machinery – Hydraulic breakers – Terminology and commercial specifications
CDN $115.00 Add to cart -

ISO 5157:2023 Textiles – Environmental aspects – Vocabulary
CDN $76.00 Add to cart -

ISO 6707:2022 Buildings and civil engineering works – Vocabulary – Part 3: Sustainability terms
CDN $76.00 Add to cart -

ISO 8927:1991 Earth-moving machinery – Machine availability – Vocabulary
CDN $233.00 Add to cart