ISO 6892:2015
ISO 6892:2015 Metallic materials – Tensile testing – Part 4: Method of test in liquid helium
CDN $195.00
Description
ISO 6892-4:2015 specifies the method of tensile testing of metallic materials in liquid helium (the boiling point is ?269 °C or 4,2 K, designated as 4 K) and defines the mechanical properties that can be determined.
This part of ISO 6892 may apply also to tensile testing at cryogenic temperatures (less than ?196 °C or 77 K), which requires special apparatus, smaller test pieces, and concern for serrated yielding, adiabatic heating, and strain-rate effects.
To conduct a tensile test according to this part of ISO 6892 at 4 K, the test piece installed in a cryostat is fully submerged in liquid helium (He) and tested using displacement control at a nominal strain rate of 10‚àí3 s‚àí1 or less.
NOTE The boiling point of the rare 3He isotope is 3,2 K. Usually, the tests are performed in 4He or a mixture of 3He and 4He with a high concentration of 4He. Therefore, the temperature is, as designated before, 4 K.
Edition
1
Published Date
2015-09-29
Status
PUBLISHED
Pages
13
Format 
Secure PDF
Secure – PDF details
- Save your file locally or view it via a web viewer
- Viewing permissions are restricted exclusively to the purchaser
- Device limits - 3
- Printing – Enabled only to print (1) copy
See more about our Environmental Commitment
Abstract
ISO 6892-4:2015 specifies the method of tensile testing of metallic materials in liquid helium (the boiling point is ?269 °C or 4,2 K, designated as 4 K) and defines the mechanical properties that can be determined.
This part of ISO 6892 may apply also to tensile testing at cryogenic temperatures (less than ?196 °C or 77 K), which requires special apparatus, smaller test pieces, and concern for serrated yielding, adiabatic heating, and strain-rate effects.
To conduct a tensile test according to this part of ISO 6892 at 4 K, the test piece installed in a cryostat is fully submerged in liquid helium (He) and tested using displacement control at a nominal strain rate of 10‚àí3 s‚àí1 or less.
NOTE The boiling point of the rare 3He isotope is 3,2 K. Usually, the tests are performed in 4He or a mixture of 3He and 4He with a high concentration of 4He. Therefore, the temperature is, as designated before, 4 K.
Previous Editions
Can’t find what you are looking for?
Please contact us at:
Related Documents
-

ISO 7039:2024 Metallic materials – Tensile testing – Method for evaluating the susceptibility of materials to the effects of high-pressure gas within hollow test pieces
CDN $131.00 Add to cart -

ISO 4507:2000 Sintered ferrous materials, carburized or carbonitrided – Determination and verification of case-hardening depth by a micro-hardness test
CDN $86.00 Add to cart -

ISO 3995:2023 Metallic powders – Determination of green strength by transverse rupture of rectangular compacts
CDN $131.00 Add to cart -

ISO 3312:1987 Sintered metal materials and hardmetals – Determination of Young modulus
CDN $86.00 Add to cart