ISO 6957:1988
ISO 6957:1988 Copper alloys – Ammonia test for stress corrosion resistance
CDN $76.00
Description
Specifies a test, using an ammoniacal atmosphere, for the detection of applied or residual stresses which can cause failure of the material in service or storage through stress corrosion cracking. The severity of the method can be regulated by changing the pH value. In an informative annex, recommendations are given for the choice of pH-values.
Edition
1
Published Date
1988-09-15
Status
PUBLISHED
Pages
3
Format 
Secure PDF
Secure – PDF details
- Save your file locally or view it via a web viewer
- Viewing permissions are restricted exclusively to the purchaser
- Device limits - 3
- Printing – Enabled only to print (1) copy
See more about our Environmental Commitment
Abstract
Specifies a test, using an ammoniacal atmosphere, for the detection of applied or residual stresses which can cause failure of the material in service or storage through stress corrosion cracking. The severity of the method can be regulated by changing the pH value. In an informative annex, recommendations are given for the choice of pH-values.
Previous Editions
Can’t find what you are looking for?
Please contact us at:
Related Documents
-

ISO 11844:2020 Corrosion of metals and alloys – Classification of low corrosivity of indoor atmospheres – Part 2: Determination of corrosion attack in indoor atmospheres
CDN $173.00 Add to cart -

ISO 22410:2020 Corrosion of metals and alloys – Electrochemical measurement of ion transfer resistance to characterize the protective rust layer on weathering steel
CDN $173.00 Add to cart -

ISO 17475:2005 Corrosion of metals and alloys – Electrochemical test methods – Guidelines for conducting potentiostatic and potentiodynamic polarization measurements
CDN $173.00 Add to cart -

ISO 21207:2015 Corrosion tests in artificial atmospheres – Accelerated corrosion tests involving alternate exposure to corrosion-promoting gases, neutral salt-spray and drying
CDN $115.00 Add to cart