ISO 7500:2006
ISO 7500:2006 Metallic materials – Verification of static uniaxial testing machines – Part 2: Tension creep testing machines – Verification of the applied force
CDN $173.00
Description
ISO 7500-2:2006 specifies the verification of testing machines used for uniaxial creep testing in tension in accordance with ISO 204.
The verification consists of
- a general inspection of the testing machine, and
- a verification of the force applied by the testing machine.
ISO 7500-2:2006 applies to dead-weight machines, lever-type creep testing machines and direct-spring-loading machines.
Machines with a force-measuring system should be verified in accordance with ISO 7500-1.
Edition
2
Published Date
2006-12-05
Status
PUBLISHED
Pages
17
Format 
Secure PDF
Secure – PDF details
- Save your file locally or view it via a web viewer
- Viewing permissions are restricted exclusively to the purchaser
- Device limits - 3
- Printing – Enabled only to print (1) copy
See more about our Environmental Commitment
Abstract
ISO 7500-2:2006 specifies the verification of testing machines used for uniaxial creep testing in tension in accordance with ISO 204.
The verification consists of
- a general inspection of the testing machine, and
- a verification of the force applied by the testing machine.
ISO 7500-2:2006 applies to dead-weight machines, lever-type creep testing machines and direct-spring-loading machines.
Machines with a force-measuring system should be verified in accordance with ISO 7500-1.
Previous Editions
Can’t find what you are looking for?
Please contact us at:
Related Documents
-

ISO 2739:2012 Sintered metal bushings – Determination of radial crushing strength
CDN $76.00 Add to cart -

ISO 7039:2024 Metallic materials – Tensile testing – Method for evaluating the susceptibility of materials to the effects of high-pressure gas within hollow test pieces
CDN $115.00 Add to cart -

ISO 6507:2023 Metallic materials – Vickers hardness test – Part 1: Test method
CDN $273.00 Add to cart -

ISO 3738:1982 Hardmetals – Rockwell hardness test (scale A) – Part 1: Test method
CDN $76.00 Add to cart