Your cart is currently empty!

ISO 8994:2018
ISO 8994:2018 Anodizing of aluminium and its alloys – Rating system for the evaluation of pitting corrosion – Grid method
CDN $76.00
Description
This document specifies a grid rating system that provides a means of defining levels of performance of anodic oxidation coatings on aluminium and its alloys that have been subjected to corrosion tests.
This rating system is applicable to pitting corrosion resulting from
– accelerated tests,
– exposure to corrosive environments, and
– practical service tests.
This document takes into account only pitting corrosion of the basis metal resulting from penetration of the protective anodic oxidation coating.
NOTE 1 ISO 8993[1] describes a similar rating system based on defined chart scales.
NOTE 2 The grid rating system is frequently used for rating the results of short-term corrosion tests for relatively thin anodic oxidation coating, such as those used in the automotive industry.
Edition
3
Published Date
2018-11-12
Status
PUBLISHED
Pages
4
Format 
Secure PDF
Secure – PDF details
- Save your file locally or view it via a web viewer
- Viewing permissions are restricted exclusively to the purchaser
- Device limits - 3
- Printing – Enabled only to print (1) copy
See more about our Environmental Commitment

Abstract
This document specifies a grid rating system that provides a means of defining levels of performance of anodic oxidation coatings on aluminium and its alloys that have been subjected to corrosion tests.
This rating system is applicable to pitting corrosion resulting from
- accelerated tests,
- exposure to corrosive environments, and
- practical service tests.
This document takes into account only pitting corrosion of the basis metal resulting from penetration of the protective anodic oxidation coating.
NOTE 1 ISO 8993[1] describes a similar rating system based on defined chart scales.
NOTE 2 The grid rating system is frequently used for rating the results of short-term corrosion tests for relatively thin anodic oxidation coating, such as those used in the automotive industry.
Previous Editions
Can’t find what you are looking for?
Please contact us at:
Related Documents
-
ISO 612:1978 Road vehicles – Dimensions of motor vehicles and towed vehicles – Terms and definitions
CDN $173.00 Add to cart -
ISO 4006:1991 Measurement of fluid flow in closed conduits – Vocabulary and symbols
CDN $351.00 Add to cart -
ISO 80004:2011 Nanotechnologies – Vocabulary – Part 5: Nano/bio interface
CDN $76.00 Add to cart -
ISO 80004:2020 Nanotechnologies – Vocabulary – Part 3: Carbon nano-objects
CDN $76.00 Add to cart