ISO 11357-5:2025
ISO 11357-5:2025 Plastics — Differential scanning calorimetry (DSC) — Part 5: Determination of characteristic reaction-curve temperatures and times, enthalpy of reaction and degree of conversion
CDN $125.00
This publication was last reviewed and confirmed in 2025.
Plastics — Differential scanning calorimetry (DSC) — Part 5: Determination of characteristic reaction-curve temperatures and times, enthalpy of reaction and degree of conversion
Description
This document specifies a method for the determination of reaction temperatures and times, enthalpies of reaction, and degrees of conversion using conventional differential scanning calorimetry (DSC) as specified in ISO 11357-1.
The method applies to monomers, prepolymers, and polymers in the solid or liquid state. The material can contain fillers and/or initiators in the solid or liquid state.
This document is not applicable to fast DSC as specified in ISO 23976.[ REF Reference_ref_2 r h 1
08D0C9EA79F9BACE118C8200AA004BA90B0200000008000000100000005200650066006500720065006E00630065005F007200650066005F0032000000
]
Edition
3
Published Date
2026-06-18
Status
PUBLISHED
Pages
10
Format 
Secure PDF
Secure – PDF details
- Save your file locally or view it via a web viewer
- Viewing permissions are restricted exclusively to the purchaser
- Device limits - 3
- Printing – Enabled only to print (1) copy
See more about our Environmental Commitment
Abstract
This document specifies a method for the determination of reaction temperatures and times, enthalpies of reaction, and degrees of conversion using conventional differential scanning calorimetry (DSC) as specified in ISO 11357-1.
The method applies to monomers, prepolymers, and polymers in the solid or liquid state. The material can contain fillers and/or initiators in the solid or liquid state.
This document is not applicable to fast DSC as specified in ISO 23976.[ REF Reference_ref_2 r h 1 08D0C9EA79F9BACE118C8200AA004BA90B0200000008000000100000005200650066006500720065006E00630065005F007200650066005F0032000000 ]
Previous Editions
Can’t find what you are looking for?
Please contact us at:
Related Documents
-

ISO 3833:1977 Road vehicles – Types – Terms and definitions
CDN $124.00 Add to cart -

ISO 80004:2021 Nanotechnologies – Vocabulary – Part 6: Nano-object characterization
CDN $82.00 Add to cart -

ISO 16840:2006 Wheelchair seating – Part 1: Vocabulary, reference axis convention and measures for body segments, posture and postural support surfaces
CDN $379.00 Add to cart -

ISO 5078:2025 Management of terminology resources – Terminology extraction
CDN $251.00 Add to cart