ISO 15614-2:2025
ISO 15614-2:2025 Specification and qualification of welding procedures for metallic materials — Welding procedure test — Part 2: Arc welding of aluminium and its alloys
CDN $251.00
This publication was last reviewed and confirmed in 2025.
Specification and qualification of welding procedures for metallic materials — Welding procedure test — Part 2: Arc welding of aluminium and its alloys
Description
This document specifies how a preliminary welding procedure specification (pWPS) is qualified by welding procedure tests.
This document applies to production welding, repair welding and build-up welding.
This document defines the conditions for the execution of welding procedure tests and the range of qualification for welding procedures for all practical welding operations within the qualification of this document.
This document applies to the arc welding of wrought and cast aluminium and its alloys. In this document the term aluminium stands for aluminium and for aluminium alloys.
This document does not apply to finishing welding of aluminium castings, which is addressed in ISO 15614-4.
Arc welding of aluminium is covered by the following welding processes in accordance with ISO 4063:2023:
131 — MIG welding with solid wire electrode;
141 — TIG welding with solid filler material (wire/rod);
142 — Autogenous TIG welding;
15 — plasma arc welding.
Edition
2
Published Date
2026-06-18
Status
PUBLISHED
Pages
26
Format 
Secure PDF
Secure – PDF details
- Save your file locally or view it via a web viewer
- Viewing permissions are restricted exclusively to the purchaser
- Device limits - 3
- Printing – Enabled only to print (1) copy
See more about our Environmental Commitment
Abstract
This document specifies how a preliminary welding procedure specification (pWPS) is qualified by welding procedure tests.
This document applies to production welding, repair welding and build-up welding.
This document defines the conditions for the execution of welding procedure tests and the range of qualification for welding procedures for all practical welding operations within the qualification of this document.
This document applies to the arc welding of wrought and cast aluminium and its alloys. In this document the term aluminium stands for aluminium and for aluminium alloys.
This document does not apply to finishing welding of aluminium castings, which is addressed in ISO 15614-4.
Arc welding of aluminium is covered by the following welding processes in accordance with ISO 4063:2023:
131 — MIG welding with solid wire electrode;
141 — TIG welding with solid filler material (wire/rod);
142 — Autogenous TIG welding;
15 — plasma arc welding.
Previous Editions
Can’t find what you are looking for?
Please contact us at:
Related Documents
-

ISO 15011:2009 Health and safety in welding and allied processes – Laboratory method for sampling fume and gases – Part 3: Determination of ozone emission rate during arc welding
CDN $192.00 Add to cart -

ISO 15011:2012 Health and safety in welding and allied processes – Laboratory method for sampling fume and gases – Part 6: Procedure for quantitative determination of fume and gases from resistance spot welding
CDN $259.00 Add to cart -

ISO 25901:2016 Welding and allied processes – Vocabulary – Part 4: Arc welding
CDN $85.00 Add to cart -

ISO 15011:2011 Health and safety in welding and allied processes – Laboratory method for sampling fume and gases – Part 5: Identification of thermal-degradation products generated when welding or cutting through products composed wholly or partly of organic materials using pyrolysis-gas chromatography-mass spectrometry
CDN $192.00 Add to cart