ISO 15614-9:2025

ISO 15614-9:2025 Specification and qualification of welding procedures for metallic materials — Welding procedure test — Part 9: Underwater hyperbaric wet welding

CDN $337.00

This publication was last reviewed and confirmed in 2025.

Specification and qualification of welding procedures for metallic materials — Welding procedure test — Part 9: Underwater hyperbaric wet welding

SKU: 40bc6614d828 Categories: ,

Description

This document specifies how a preliminary welding procedure specification (pWPS) is qualified by welding procedure tests.

This document is applicable to production welding and repair welding.

This document is applicable to fusion welding of steels covered by groups 1, 2, 3 and 8 in accordance with ISO 15608 in a hyperbaric wet environment.

This document is applicable to the following welding processes, in accordance with ISO 4063:2023, applicable in hyperbaric wet environments:

—     111 manual metal arc welding (metal arc welding with covered electrode);

—     114 self-shielded tubular-cored arc welding.

The principles of this document can be applied to other steel groups and fusion welding processes not listed.

This document specifies three weld quality levels, A, B, and Z in order to permit application to a wide range of weldments. Each weld quality level defines a set of criteria for weldment properties that are established during qualification.

This document does not address the selection of the weld quality level to meet the requirements of a particular application.

Edition

1

Published Date

2026-06-18

Status

PUBLISHED

Pages

42

Language Detail Icon

English

Format Secure Icon

Secure PDF

Abstract

This document specifies how a preliminary welding procedure specification (pWPS) is qualified by welding procedure tests.

This document is applicable to production welding and repair welding.

This document is applicable to fusion welding of steels covered by groups 1, 2, 3 and 8 in accordance with ISO 15608 in a hyperbaric wet environment.

This document is applicable to the following welding processes, in accordance with ISO 4063:2023, applicable in hyperbaric wet environments:

—     111 manual metal arc welding (metal arc welding with covered electrode);

—     114 self-shielded tubular-cored arc welding.

The principles of this document can be applied to other steel groups and fusion welding processes not listed.

This document specifies three weld quality levels, A, B, and Z in order to permit application to a wide range of weldments. Each weld quality level defines a set of criteria for weldment properties that are established during qualification.

This document does not address the selection of the weld quality level to meet the requirements of a particular application.