API RP 15SIH, 2nd Edition: Installation and Handling of Spoolable Reinforced Plastic Line Pipe

$

158

BUY NOW

Placeholder headline

This is just a placeholder headline

API RP 754, 4th Edition: Process Safety Performance Indicators for the Refining and Petrochemical Industries

$

393

BUY NOW

Placeholder headline

This is just a placeholder headline

ASME B31.1-2020: Power Piping

$

668

BUY NOW

Placeholder headline

This is just a placeholder headline

ASME B31.1-2022: Power Piping

$

668

BUY NOW

ISO 7529:2017

ISO 7529:2017 Nickel alloys – Determination of chromium content – Potentiometric titration method with ammonium iron(II) sulfate

CDN $85.00

SKU: bcbb8bd320f0 Category:

Description

ISO 7529:2017 specifies a potentiometric titration method for the determination of chromium content in nickel alloys which do not contain insoluble carbides and which have a vanadium content less than a mass fraction of 0,2 %. The method is applicable to chromium contents between a mass fraction of 5 % and a mass fraction of 22 %.

Vanadium, which can be present as an impurity in the alloy, will give a positive bias interference. However, at a level of a mass fraction of 0,2 %, this bias is equivalent to a mass fraction of 0,068 % chromium, which is about half the reproducibility of the method.

Edition

2

Published Date

2017-10-27

Status

PUBLISHED

Pages

5

Language Detail Icon

English

Format Secure Icon

Secure PDF

Abstract

ISO 7529:2017 specifies a potentiometric titration method for the determination of chromium content in nickel alloys which do not contain insoluble carbides and which have a vanadium content less than a mass fraction of 0,2 %. The method is applicable to chromium contents between a mass fraction of 5 % and a mass fraction of 22 %.

Vanadium, which can be present as an impurity in the alloy, will give a positive bias interference. However, at a level of a mass fraction of 0,2 %, this bias is equivalent to a mass fraction of 0,068 % chromium, which is about half the reproducibility of the method.