Your cart is currently empty!

ISO 14322:2018
ISO 14322:2018 Plastics – Epoxy resins – Determination of degree of crosslinking of crosslinked epoxy resins by differential scanning calorimetry (DSC)
CDN $115.00
Description
This document specifies a method whereby the heat of reaction generated during epoxy resin crosslinking is measured by differential scanning calorimetry (DSC). The degree of crosslinking is determined based on this result.
This method is applicable to epoxy resin systems with a moderate or slow crosslinking-reaction speed. It might not be applicable to systems with a fast crosslinking-reaction speed at ambient temperature.
Edition
2
Published Date
2018-07-19
Status
PUBLISHED
Pages
8
Format 
Secure PDF
Secure – PDF details
- Save your file locally or view it via a web viewer
- Viewing permissions are restricted exclusively to the purchaser
- Device limits - 3
- Printing – Enabled only to print (1) copy
See more about our Environmental Commitment

Abstract
This document specifies a method whereby the heat of reaction generated during epoxy resin crosslinking is measured by differential scanning calorimetry (DSC). The degree of crosslinking is determined based on this result.
This method is applicable to epoxy resin systems with a moderate or slow crosslinking-reaction speed. It might not be applicable to systems with a fast crosslinking-reaction speed at ambient temperature.
Previous Editions
Can’t find what you are looking for?
Please contact us at:
Related Documents
-
ISO 21120:2025 Machinery for forestry – Forestry mulching equipment – Terms, definitions and commercial specifications
0 out of 5CDN $173.00 Add to cart -
ISO 21625:2020 Vocabulary related to bamboo and bamboo products
0 out of 5CDN $76.00 Add to cart -
ISO 20480:2021 Fine bubble technology – General principles for usage and measurement of fine bubbles – Part 3: Methods for generating fine bubbles
0 out of 5CDN $173.00 Add to cart -
ISO 4125:1991 Dry fruits and dried fruits – Definitions and nomenclature
0 out of 5CDN $76.00 Add to cart