REGISTER

FR
Search
×
FR

Placeholder headline

This is just a placeholder headline

API RP 1173: Pipeline Safety Management Systems

$

167

BUY NOW

Placeholder headline

This is just a placeholder headline

API RP 1173: Pipeline Safety Management Systems : Errata 1

$

0

BUY NOW

Placeholder headline

This is just a placeholder headline

API RP 11S2: Electric Submersible Pump Testing: Edition 3

$

158

BUY NOW

Placeholder headline

This is just a placeholder headline

API SPEC 14L: Lock Mandrels and Landing Nipples : Reaffirmed

$

273

BUY NOW

Placeholder headline

This is just a placeholder headline

API SPEC 20F: Corrosion Resistant Bolting for Use in the Petroleum and Natural Gas Industries : Reaffirmed

$

169

BUY NOW

Placeholder headline

This is just a placeholder headline

API TR 5NCL Nickel Content Limits for API 5CT Sour Service Products

$

149

BUY NOW

Placeholder headline

This is just a placeholder headline

API SPEC 19ICD: Inflow Control Devices : Reaffirmed

$

189

BUY NOW

ISO 19993:2020

ISO 19993:2020 Timber structures – Glued laminated timber – Face and edge joint cleavage test

CDN $76.00

SKU: a5b355f87598 Categories: ,

Description

This document specifies methods of evaluating the effectiveness of glued laminated timber face and edge bonds within a manufacturing plant by cleaving of the glue line in both dry and wet conditions. It is not intended that it be used for initial type testing where cyclic delamination or block shear is preferred. It is based on the principle that, provided minimum wood failure percentages are met, then the bond strength exceeds the perpendicular to the grain tension strength of the under-lying substrate and therefore the bond is not the weak element limiting the integrity of a glulam assembly.

Edition

2

Published Date

2020-04-14

Status

PUBLISHED

Pages

5

Language Detail Icon

English

Format Secure Icon

Secure PDF

Abstract

This document specifies methods of evaluating the effectiveness of glued laminated timber face and edge bonds within a manufacturing plant by cleaving of the glue line in both dry and wet conditions. It is not intended that it be used for initial type testing where cyclic delamination or block shear is preferred. It is based on the principle that, provided minimum wood failure percentages are met, then the bond strength exceeds the perpendicular to the grain tension strength of the under-lying substrate and therefore the bond is not the weak element limiting the integrity of a glulam assembly.