ISO 21746:2019
ISO 21746:2019 Composites and metal assemblies – Galvanic corrosion tests of carbon fibre reinforced plastics (CFRPs) related bonded or fastened structures in artificial atmospheres – Salt spray tests
CDN $233.00
Description
This document specifies the apparatus, the reagents and the procedure to be used in conducting the neutral salt spray (NSS), acetic acid salt spray (AASS) and copper-accelerated acetic acid salt spray (CASS) tests for assessment of the galvanic corrosion resistance of joints and bonded structures between carbon fibre reinforced plastics (CFRPs) and metallic materials, with or without permanent or temporary insulation for the galvanic current.
Edition
1
Published Date
2019-04-26
Status
PUBLISHED
Pages
19
Format 
Secure PDF
Secure – PDF details
- Save your file locally or view it via a web viewer
- Viewing permissions are restricted exclusively to the purchaser
- Device limits - 3
- Printing – Enabled only to print (1) copy
See more about our Environmental Commitment

Abstract
This document specifies the apparatus, the reagents and the procedure to be used in conducting the neutral salt spray (NSS), acetic acid salt spray (AASS) and copper-accelerated acetic acid salt spray (CASS) tests for assessment of the galvanic corrosion resistance of joints and bonded structures between carbon fibre reinforced plastics (CFRPs) and metallic materials, with or without permanent or temporary insulation for the galvanic current.
Previous Editions
Can’t find what you are looking for?
Please contact us at:
Related Documents
-
ISO 8384:2019 Ships and marine technology – Dredgers – Vocabulary
0 out of 5CDN $76.00 Add to cart -
ISO 80004:2020 Nanotechnologies – Vocabulary – Part 3: Carbon nano-objects
0 out of 5CDN $76.00 Add to cart -
ISO 2574:1994 Aircraft – Electrical cables – Identification marking
0 out of 5CDN $115.00 Add to cart -
ISO 612:1978 Road vehicles – Dimensions of motor vehicles and towed vehicles – Terms and definitions
0 out of 5CDN $173.00 Add to cart