This document describes a method for the determination of the glass transition temperature (Tg) of kraft lignin. The procedure utilizes differential scanning calorimetry (DSC).
This procedure is applicable to solid lignins (e.g., powdered form) isolated using different isolation techniques (e.g., acidification with hydrochloric acid, sulfuric acid, etc., and carbonation using gaseous carbon dioxide) from the spent liquor (black liquor) generated from the kraft pulping process.
It does not apply to raw black liquor and lignin in the alkali form, (lignin that is separated from wood chips and dissolved in sodium sulfide and sodium hydroxide liquor such as that originating from black liquor).
Edition
1
Published Date
2024-09-30
Status
PUBLISHED
Pages
7
Format 
Secure PDF
Secure – PDF details
- Save your file locally or view it via a web viewer
- Viewing permissions are restricted exclusively to the purchaser
- Device limits - 3
- Printing – Enabled only to print (1) copy
See more about our Environmental Commitment

Abstract
This document describes a method for the determination of the glass transition temperature (Tg) of kraft lignin. The procedure utilizes differential scanning calorimetry (DSC).
This procedure is applicable to solid lignins (e.g., powdered form) isolated using different isolation techniques (e.g., acidification with hydrochloric acid, sulfuric acid, etc., and carbonation using gaseous carbon dioxide) from the spent liquor (black liquor) generated from the kraft pulping process.
It does not apply to raw black liquor and lignin in the alkali form, (lignin that is separated from wood chips and dissolved in sodium sulfide and sodium hydroxide liquor such as that originating from black liquor).
Previous Editions
Can’t find what you are looking for?
Please contact us at:
Related Documents
-
ISO 4006:1991 Measurement of fluid flow in closed conduits – Vocabulary and symbols
0 out of 5CDN $351.00 Add to cart -
ISO 2574:1994 Aircraft – Electrical cables – Identification marking
0 out of 5CDN $115.00 Add to cart -
ISO 1176:1990 Road vehicles – Masses – Vocabulary and codes
0 out of 5CDN $115.00 Add to cart -
ISO 80004:2011 Nanotechnologies – Vocabulary – Part 5: Nano/bio interface
0 out of 5CDN $76.00 Add to cart