Your cart is currently empty!
“ISO 9488:2022 Solar energy – Vocabulary” has been added to your cart. View cart

ISO 24144:2023
ISO 24144:2023 Thermal insulation – Test methods for specific heat capacity of thermal insulation for buildings in the high temperature range – Differential scanning calorimetry (DSC) method
CDN $233.00
SKU: dc9bee627eef
Categories: ICS:91.120.10, SUSTAINABLE_DEVELOPMENT_GOAL:7
Description
This document specifies test methods for specific heat capacity under high temperature conditions from the normal temperature range to 1 600 K for insulation materials for buildings using the differential scanning calorimetry (DSC) method.
Edition
1
Published Date
2023-01-10
Status
PUBLISHED
Pages
21
Format 
Secure PDF
Secure – PDF details
- Save your file locally or view it via a web viewer
- Viewing permissions are restricted exclusively to the purchaser
- Device limits - 3
- Printing – Enabled only to print (1) copy
See more about our Environmental Commitment

Abstract
This document specifies test methods for specific heat capacity under high temperature conditions from the normal temperature range to 1 600 K for insulation materials for buildings using the differential scanning calorimetry (DSC) method.
Previous Editions
Can’t find what you are looking for?
Please contact us at:
Related Documents
-
ISO 37101:2016 Sustainable development in communities – Management system for sustainable development – Requirements with guidance for use
0 out of 5CDN $273.00 Add to cart -
ISO 32210:2022 Sustainable finance – Guidance on the application of sustainability principles for organizations in the financial sector
0 out of 5CDN $233.00 Add to cart -
ISO 5207:2024 Information technology – Data usage – Terminology and use cases
0 out of 5CDN $351.00 Add to cart -
ISO 20670:2023 Water reuse – Vocabulary
0 out of 5CDN $173.00 Add to cart