ISO 8057:2024 Determination of galvanic corrosion rate for assembled forms of carbon fibre reinforced plastics (CFRPs) and protection-coated metal – Electrochemical tests in neutral sodium chloride solution
CDN $173.00
Description
This document specifies the electrochemical test for determining galvanic corrosion rate of CFRPs and metal assemblies with protection-coating, subjected to the corrosive environment of electrolyte diffusion through the coating. It specifies the apparatus, the test solutions, and the procedure to be used in conducting the electrochemical tests for
a)¬†¬†¬†¬†¬†¬† the assessment of the Fick’s diffusion parameter for protective coating on metallic materials, and
b)       the estimation of the galvanic corrosion rates with the conversion of ISO 21746 coating-free sample data.
The following are intended situations of implementing an electrochemical test based on this document:
a)       when interested parties estimate the galvanic corrosion rate of bonded joints relating engineering metals with protection-coating and CFRPs of the potential drastically nobler than those of most metals, utilizing the resources of ISO 17475;
b)       when expanding CFRP-metal bonded joints applications using coatings to the fields of corrosion-sensitive environments caused by electrolytes.
It is not the intent of this document to fulfil the need for:
–¬†¬†¬†¬† omitting relevant field tests for the applications in corrosive environment;
–¬†¬†¬†¬† superimposing test data for specific applications for the range of relevant data;
–¬†¬†¬†¬† comparative testing as a means of ranking different protections with respect to corrosion rates;
–¬†¬†¬†¬† ignoring the field hazards such as erosion, abrasion, and ultraviolet irradiation.
Edition
1
Published Date
2024-01-26
Status
PUBLISHED
Pages
14
Format 
Secure PDF
Secure – PDF details
- Save your file locally or view it via a web viewer
- Viewing permissions are restricted exclusively to the purchaser
- Device limits - 3
- Printing – Enabled only to print (1) copy
See more about our Environmental Commitment

Abstract
This document specifies the electrochemical test for determining galvanic corrosion rate of CFRPs and metal assemblies with protection-coating, subjected to the corrosive environment of electrolyte diffusion through the coating. It specifies the apparatus, the test solutions, and the procedure to be used in conducting the electrochemical tests for
a)       the assessment of the Fick's diffusion parameter for protective coating on metallic materials, and
b)       the estimation of the galvanic corrosion rates with the conversion of ISO 21746 coating-free sample data.
The following are intended situations of implementing an electrochemical test based on this document:
a)       when interested parties estimate the galvanic corrosion rate of bonded joints relating engineering metals with protection-coating and CFRPs of the potential drastically nobler than those of most metals, utilizing the resources of ISO 17475;
b)       when expanding CFRP-metal bonded joints applications using coatings to the fields of corrosion-sensitive environments caused by electrolytes.
It is not the intent of this document to fulfil the need for:
-     omitting relevant field tests for the applications in corrosive environment;
-     superimposing test data for specific applications for the range of relevant data;
-     comparative testing as a means of ranking different protections with respect to corrosion rates;
-     ignoring the field hazards such as erosion, abrasion, and ultraviolet irradiation.
Previous Editions
Can’t find what you are looking for?
Please contact us at:
Related Documents
-
ISO 80004:2011 Nanotechnologies – Vocabulary – Part 7: Diagnostics and therapeutics for healthcare
0 out of 5CDN $115.00 Add to cart -
ISO 2574:1994 Aircraft – Electrical cables – Identification marking
0 out of 5CDN $115.00 Add to cart -
ISO 8927:1991 Earth-moving machinery – Machine availability – Vocabulary
0 out of 5CDN $233.00 Add to cart -
ISO 22553:2019 Paints and varnishes – Electro-deposition coatings – Part 1: Vocabulary
0 out of 5CDN $76.00 Add to cart