ISO 14322:2018 Plastics – Epoxy resins – Determination of degree of crosslinking of crosslinked epoxy resins by differential scanning calorimetry (DSC)
CDN $115.00
Description
This document specifies a method whereby the heat of reaction generated during epoxy resin crosslinking is measured by differential scanning calorimetry (DSC). The degree of crosslinking is determined based on this result.
This method is applicable to epoxy resin systems with a moderate or slow crosslinking-reaction speed. It might not be applicable to systems with a fast crosslinking-reaction speed at ambient temperature.
Edition
2
Published Date
2018-07-19
Status
PUBLISHED
Pages
8
Format 
Secure PDF
Secure – PDF details
- Save your file locally or view it via a web viewer
- Viewing permissions are restricted exclusively to the purchaser
- Device limits - 3
- Printing – Enabled only to print (1) copy
See more about our Environmental Commitment

Abstract
This document specifies a method whereby the heat of reaction generated during epoxy resin crosslinking is measured by differential scanning calorimetry (DSC). The degree of crosslinking is determined based on this result.
This method is applicable to epoxy resin systems with a moderate or slow crosslinking-reaction speed. It might not be applicable to systems with a fast crosslinking-reaction speed at ambient temperature.
Previous Editions
Can’t find what you are looking for?
Please contact us at:
Related Documents
-
ISO 5157:2023 Textiles – Environmental aspects – Vocabulary
0 out of 5CDN $76.00 Add to cart -
ISO 8927:1991 Earth-moving machinery – Machine availability – Vocabulary
0 out of 5CDN $233.00 Add to cart -
ISO 1956:1982 Fruits and vegetables – Morphological and structural terminology
0 out of 5CDN $233.00 Add to cart -
ISO 6405:2017 Earth-moving machinery – Symbols for operator controls and other displays – Part 2: Symbols for specific machines, equipment and accessories
0 out of 5CDN $351.00 Add to cart