ISO 21746:2019
ISO 21746:2019 Composites and metal assemblies – Galvanic corrosion tests of carbon fibre reinforced plastics (CFRPs) related bonded or fastened structures in artificial atmospheres – Salt spray tests
CDN $233.00
Description
This document specifies the apparatus, the reagents and the procedure to be used in conducting the neutral salt spray (NSS), acetic acid salt spray (AASS) and copper-accelerated acetic acid salt spray (CASS) tests for assessment of the galvanic corrosion resistance of joints and bonded structures between carbon fibre reinforced plastics (CFRPs) and metallic materials, with or without permanent or temporary insulation for the galvanic current.
Edition
1
Published Date
2019-04-26
Status
PUBLISHED
Pages
19
Format 
Secure PDF
Secure – PDF details
- Save your file locally or view it via a web viewer
- Viewing permissions are restricted exclusively to the purchaser
- Device limits - 3
- Printing – Enabled only to print (1) copy
See more about our Environmental Commitment

Abstract
This document specifies the apparatus, the reagents and the procedure to be used in conducting the neutral salt spray (NSS), acetic acid salt spray (AASS) and copper-accelerated acetic acid salt spray (CASS) tests for assessment of the galvanic corrosion resistance of joints and bonded structures between carbon fibre reinforced plastics (CFRPs) and metallic materials, with or without permanent or temporary insulation for the galvanic current.
Previous Editions
Can’t find what you are looking for?
Please contact us at:
Related Documents
-
ISO 80004:2011 Nanotechnologies – Vocabulary – Part 5: Nano/bio interface
0 out of 5CDN $76.00 Add to cart -
ISO 612:1978 Road vehicles – Dimensions of motor vehicles and towed vehicles – Terms and definitions
0 out of 5CDN $173.00 Add to cart -
ISO 5078:2025 Management of terminology resources – Terminology extraction
0 out of 5CDN $233.00 Add to cart -
ISO 20537:2025 Footwear – Identification of defects during visual inspection – Vocabulary
0 out of 5CDN $273.00 Add to cart