This document describes a method for the determination of the glass transition temperature (Tg) of kraft lignin. The procedure utilizes differential scanning calorimetry (DSC).
This procedure is applicable to solid lignins (e.g., powdered form) isolated using different isolation techniques (e.g., acidification with hydrochloric acid, sulfuric acid, etc., and carbonation using gaseous carbon dioxide) from the spent liquor (black liquor) generated from the kraft pulping process.
It does not apply to raw black liquor and lignin in the alkali form, (lignin that is separated from wood chips and dissolved in sodium sulfide and sodium hydroxide liquor such as that originating from black liquor).
Edition
1
Published Date
2024-09-30
Status
PUBLISHED
Pages
7
Format 
Secure PDF
Secure – PDF details
- Save your file locally or view it via a web viewer
- Viewing permissions are restricted exclusively to the purchaser
- Device limits - 3
- Printing – Enabled only to print (1) copy
See more about our Environmental Commitment

Abstract
This document describes a method for the determination of the glass transition temperature (Tg) of kraft lignin. The procedure utilizes differential scanning calorimetry (DSC).
This procedure is applicable to solid lignins (e.g., powdered form) isolated using different isolation techniques (e.g., acidification with hydrochloric acid, sulfuric acid, etc., and carbonation using gaseous carbon dioxide) from the spent liquor (black liquor) generated from the kraft pulping process.
It does not apply to raw black liquor and lignin in the alkali form, (lignin that is separated from wood chips and dissolved in sodium sulfide and sodium hydroxide liquor such as that originating from black liquor).
Previous Editions
Can’t find what you are looking for?
Please contact us at:
Related Documents
-
ISO 612:1978 Road vehicles – Dimensions of motor vehicles and towed vehicles – Terms and definitions
0 out of 5CDN $173.00 Add to cart -
ISO 80004:2021 Nanotechnologies – Vocabulary – Part 6: Nano-object characterization
0 out of 5CDN $76.00 Add to cart -
ISO 14416:2003 Information and documentation – Requirements for binding of books, periodicals, serials and other paper documents for archive and library use – Methods and materials
0 out of 5CDN $273.00 Add to cart -
ISO 80000:2025 Quantities and units – Part 13: Information science and technology
0 out of 5CDN $203.00 Add to cart