REGISTER

FR
Search
×
FR

Placeholder headline

This is just a placeholder headline

API RP 1173: Pipeline Safety Management Systems

$

167

BUY NOW

Placeholder headline

This is just a placeholder headline

API RP 1173: Pipeline Safety Management Systems : Errata 1

$

0

BUY NOW

Placeholder headline

This is just a placeholder headline

API RP 11S2: Electric Submersible Pump Testing: Edition 3

$

158

BUY NOW

Placeholder headline

This is just a placeholder headline

API SPEC 14L: Lock Mandrels and Landing Nipples : Reaffirmed

$

273

BUY NOW

Placeholder headline

This is just a placeholder headline

API SPEC 20F: Corrosion Resistant Bolting for Use in the Petroleum and Natural Gas Industries : Reaffirmed

$

169

BUY NOW

Placeholder headline

This is just a placeholder headline

API TR 5NCL Nickel Content Limits for API 5CT Sour Service Products

$

149

BUY NOW

Placeholder headline

This is just a placeholder headline

API SPEC 19ICD: Inflow Control Devices : Reaffirmed

$

189

BUY NOW

ISO 22206:2024

ISO 22206:2024 Kraft lignin – Glass transition temperature by differential scanning calorimetry

CDN $115.00

Description

This document describes a method for the determination of the glass transition temperature (Tg) of kraft lignin. The procedure utilizes differential scanning calorimetry (DSC).

This procedure is applicable to solid lignins (e.g., powdered form) isolated using different isolation techniques (e.g., acidification with hydrochloric acid, sulfuric acid, etc., and carbonation using gaseous carbon dioxide) from the spent liquor (black liquor) generated from the kraft pulping process.

It does not apply to raw black liquor and lignin in the alkali form, (lignin that is separated from wood chips and dissolved in sodium sulfide and sodium hydroxide liquor such as that originating from black liquor).

Edition

1

Published Date

2024-09-30

Status

PUBLISHED

Pages

7

Language Detail Icon

English

Format Secure Icon

Secure PDF

Abstract

This document describes a method for the determination of the glass transition temperature (Tg) of kraft lignin. The procedure utilizes differential scanning calorimetry (DSC).

This procedure is applicable to solid lignins (e.g., powdered form) isolated using different isolation techniques (e.g., acidification with hydrochloric acid, sulfuric acid, etc., and carbonation using gaseous carbon dioxide) from the spent liquor (black liquor) generated from the kraft pulping process.

It does not apply to raw black liquor and lignin in the alkali form, (lignin that is separated from wood chips and dissolved in sodium sulfide and sodium hydroxide liquor such as that originating from black liquor).