ISO 22206:2024
ISO 22206:2024 Kraft lignin – Glass transition temperature by differential scanning calorimetry
CDN $115.00
Description
This document describes a method for the determination of the glass transition temperature (Tg) of kraft lignin. The procedure utilizes differential scanning calorimetry (DSC).
This procedure is applicable to solid lignins (e.g., powdered form) isolated using different isolation techniques (e.g., acidification with hydrochloric acid, sulfuric acid, etc., and carbonation using gaseous carbon dioxide) from the spent liquor (black liquor) generated from the kraft pulping process.
It does not apply to raw black liquor and lignin in the alkali form, (lignin that is separated from wood chips and dissolved in sodium sulfide and sodium hydroxide liquor such as that originating from black liquor).
Edition
1
Published Date
2024-09-30
Status
PUBLISHED
Pages
7
Format 
Secure PDF
Secure – PDF details
- Save your file locally or view it via a web viewer
- Viewing permissions are restricted exclusively to the purchaser
- Device limits - 3
- Printing – Enabled only to print (1) copy
See more about our Environmental Commitment

Abstract
This document describes a method for the determination of the glass transition temperature (Tg) of kraft lignin. The procedure utilizes differential scanning calorimetry (DSC).
This procedure is applicable to solid lignins (e.g., powdered form) isolated using different isolation techniques (e.g., acidification with hydrochloric acid, sulfuric acid, etc., and carbonation using gaseous carbon dioxide) from the spent liquor (black liquor) generated from the kraft pulping process.
It does not apply to raw black liquor and lignin in the alkali form, (lignin that is separated from wood chips and dissolved in sodium sulfide and sodium hydroxide liquor such as that originating from black liquor).
Previous Editions
Can’t find what you are looking for?
Please contact us at:
Related Documents
-
ISO 15424:2025 Information technology – Automatic identification and data capture techniques – Data carrier identifiers (including symbology identifiers)
0 out of 5CDN $233.00 Add to cart -
ISO 4006:1991 Measurement of fluid flow in closed conduits – Vocabulary and symbols
0 out of 5CDN $351.00 Add to cart -
ISO 80004:2020 Nanotechnologies – Vocabulary – Part 8: Nanomanufacturing processes
0 out of 5CDN $76.00 Add to cart -
ISO 8384:2019 Ships and marine technology – Dredgers – Vocabulary
0 out of 5CDN $76.00 Add to cart