ISO 24144:2023 Thermal insulation – Test methods for specific heat capacity of thermal insulation for buildings in the high temperature range – Differential scanning calorimetry (DSC) method
CDN $233.00
SKU: dc9bee627eef
Categories: ICS:91.120.10, SUSTAINABLE_DEVELOPMENT_GOAL:7
Description
This document specifies test methods for specific heat capacity under high temperature conditions from the normal temperature range to 1 600 K for insulation materials for buildings using the differential scanning calorimetry (DSC) method.
Edition
1
Published Date
2023-01-10
Status
PUBLISHED
Pages
21
Format 
Secure PDF
Secure – PDF details
- Save your file locally or view it via a web viewer
- Viewing permissions are restricted exclusively to the purchaser
- Device limits - 3
- Printing – Enabled only to print (1) copy
See more about our Environmental Commitment

Abstract
This document specifies test methods for specific heat capacity under high temperature conditions from the normal temperature range to 1 600 K for insulation materials for buildings using the differential scanning calorimetry (DSC) method.
Previous Editions
Can’t find what you are looking for?
Please contact us at:
Related Documents
-
ISO 5207:2024 Information technology – Data usage – Terminology and use cases
0 out of 5CDN $351.00 Add to cart -
ISO 20480:2017 Fine bubble technology – General principles for usage and measurement of fine bubbles – Part 1: Terminology
0 out of 5CDN $76.00 Add to cart -
ISO 21276:2018 Clean cookstoves and clean cooking solutions – Vocabulary
0 out of 5CDN $76.00 Add to cart -
ISO 21637:2020 Solid recovered fuels – Vocabulary
0 out of 5CDN $76.00 Add to cart