Your cart is currently empty!
“ISO 20480:2017 Fine bubble technology – General principles for usage and measurement of fine bubbles – Part 1: Terminology” has been added to your cart. View cart

ISO 24144:2023
ISO 24144:2023 Thermal insulation – Test methods for specific heat capacity of thermal insulation for buildings in the high temperature range – Differential scanning calorimetry (DSC) method
CDN $233.00
SKU: dc9bee627eef
Categories: ICS:91.120.10, SUSTAINABLE_DEVELOPMENT_GOAL:7
Description
This document specifies test methods for specific heat capacity under high temperature conditions from the normal temperature range to 1 600 K for insulation materials for buildings using the differential scanning calorimetry (DSC) method.
Edition
1
Published Date
2023-01-10
Status
PUBLISHED
Pages
21
Format 
Secure PDF
Secure – PDF details
- Save your file locally or view it via a web viewer
- Viewing permissions are restricted exclusively to the purchaser
- Device limits - 3
- Printing – Enabled only to print (1) copy
See more about our Environmental Commitment

Abstract
This document specifies test methods for specific heat capacity under high temperature conditions from the normal temperature range to 1 600 K for insulation materials for buildings using the differential scanning calorimetry (DSC) method.
Previous Editions
Can’t find what you are looking for?
Please contact us at:
Related Documents
-
ISO 22578:2024 Graphical symbols – Safety colours and safety signs – Part 2: Measurement of photopic luminance of phosphorescent components used in a natural disaster safety way guidance system
0 out of 5CDN $76.00 Add to cart -
ISO 20670:2023 Water reuse – Vocabulary
0 out of 5CDN $173.00 Add to cart -
ISO 15081:2011 Agricultural equipment – Graphical symbols for pressurized irrigation systems
0 out of 5CDN $115.00 Add to cart -
ISO 55000:2024 Asset management – Vocabulary, overview and principles
0 out of 5CDN $173.00 Add to cart