ISO 24144:2023
ISO 24144:2023 Thermal insulation – Test methods for specific heat capacity of thermal insulation for buildings in the high temperature range – Differential scanning calorimetry (DSC) method
CDN $233.00
SKU: dc9bee627eef
Categories: ICS:91.120.10, SUSTAINABLE_DEVELOPMENT_GOAL:7
Description
This document specifies test methods for specific heat capacity under high temperature conditions from the normal temperature range to 1 600 K for insulation materials for buildings using the differential scanning calorimetry (DSC) method.
Edition
1
Published Date
2023-01-10
Status
PUBLISHED
Pages
21
Format 
Secure PDF
Secure – PDF details
- Save your file locally or view it via a web viewer
- Viewing permissions are restricted exclusively to the purchaser
- Device limits - 3
- Printing – Enabled only to print (1) copy
See more about our Environmental Commitment

Abstract
This document specifies test methods for specific heat capacity under high temperature conditions from the normal temperature range to 1 600 K for insulation materials for buildings using the differential scanning calorimetry (DSC) method.
Previous Editions
Can’t find what you are looking for?
Please contact us at:
Related Documents
-
ISO 18405:2017 Underwater acoustics – Terminology
0 out of 5CDN $76.00 Add to cart -
ISO 6084:2022 Steel and steel products – Vocabulary relating to chemical analysis
0 out of 5CDN $76.00 Add to cart -
ISO 22578:2024 Graphical symbols – Safety colours and safety signs – Part 2: Measurement of photopic luminance of phosphorescent components used in a natural disaster safety way guidance system
0 out of 5CDN $76.00 Add to cart -
ISO 5207:2024 Information technology – Data usage – Terminology and use cases
0 out of 5CDN $351.00 Add to cart